IPC-600-6012 Archives

October 2013

IPC-600-6012@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Pete Menuez <[log in to unmask]>
Reply To:
(Combined Forum of D-33a and 7-31a Subcommittees)
Date:
Mon, 7 Oct 2013 16:39:32 -0400
Content-Type:
text/plain
Parts/Attachments:
text/plain (111 lines)
Doesn't the board represent the board?  In otherwords do you need coupons since the vias are external?  

Pete

----- Original Message -----
From: Denise Chevalier [mailto:[log in to unmask]]
Sent: Monday, October 07, 2013 04:04 PM
To: [log in to unmask] <[log in to unmask]>
Subject: Re: [IPC-600-6012] a/b coupon design per 2221

Covering them would represent the board so it should be OK

-----Original Message-----
From: IPC-600-6012 [mailto:[log in to unmask]] On Behalf Of Jose A
Rios
Sent: Monday, October 07, 2013 4:01 PM
To: [log in to unmask]
Subject: Re: [IPC-600-6012] a/b coupon design per 2221

hi denise, we dont either, but if you have a design where all vias for a
via represented on a coupon are covered with soldermask, we cover it
with soldermask on the coupon as well. again only if ALL vias are
covered with sm.....

Joey Rios
PWB & Process Quality Eng'r
Endicott Interconnect Technologies
1093 Clark St.
Endicott, NY 13760
Office: 607-755-5896; Cell: 607-206-3642



From:   Denise Chevalier <[log in to unmask]>
To:     <[log in to unmask]>, 
Date:   10/07/2013 03:57 PM
Subject:        Re: [IPC-600-6012] a/b coupon design per 2221
Sent by:        IPC-600-6012 <[log in to unmask]>



We don't usually put solder mask on our A/B coupons - G coupons used for
solder mask thickness, T coupon used for DFSM tented vias (usually
covered by solder mask)

-----Original Message-----
From: IPC-600-6012 [mailto:[log in to unmask]] On Behalf Of Jose A
Rios
Sent: Monday, October 07, 2013 3:29 PM
To: [log in to unmask]
Subject: [IPC-600-6012] a/b coupon design per 2221

hi all, what is the proper configuration of an ipc a/b coupon for layer
1, relative to soldermask, given the 2 designs below?? for both, the
total number of vias in the pwb is in the 10,000 - 11,000 range.
- design 1: 
- 'b' holes only (no 'a' size holes),
- all filled and cap plated,
- on layer 1, 95% of those vias are covered with soldermask, 5% have
soldermask openings hence exposed thru final finish,
- on the bottom layer, 100% of the vias have soldermask openings
- design 2:
- same as above, except only 0.1% of the vias have soldermask openings
on layer 1

leave a soldermask opening on layer 1 of the a/b's, or cover them with
soldermask?? 
include both in the coupon design, at say a 3:4 ratio (given its an a/b
theres 4 holes, 3 covered with sm, 1 uncovered)?? 
aabus??

Joey Rios
PWB & Process Quality Eng'r
Endicott Interconnect Technologies
1093 Clark St.
Endicott, NY 13760
Office: 607-755-5896; Cell: 607-206-3642

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud
service.
For more information please contact helpdesk at x2960 or
[log in to unmask]
______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud
service.
For more information please contact helpdesk at x2960 or
[log in to unmask]
______________________________________________________________________



______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud
service.
For more information please contact helpdesk at x2960 or
[log in to unmask] 
______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2