I completely agree with Patty, a board with these design rules should be a
no-brainer for any competent shop. Susan, if you want to give your supplier
a temporary method of culling bad boards while they solve their process
problems, consider electrical test. I've never done this on a double-sided
board, since the flaws are usually caught on visual inspection, but in this
case, it could buy your supplier a little bit of time to solve their
problem. If they can't tell you what went wrong and how they fixed it
pretty soon, I'd change ships (or shops).
Seth Goodman
Goodman Associates
7687 Leta Way
Verona, WI 53593-8631
Tel (608)833-9933
Fax (608)833-9966
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|