TECHNET Archives

August 1999

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Fri, 20 Aug 1999 08:56:33 +0200
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Subject:
From:
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
<C9AA15FD0636D211811B0000F8106481033CD720@FSUHHZ35>
Content-Type:
text/plain; charset=ISO-8859-1; name="Re:"
MIME-Version:
1.0
Parts/Attachments:
Re: (152 lines)
Hi Hans,
so you keep the saucers flying?
I have allways been wondering about Kester's Solder QPL list: are they
much chosen by the professionals? As such:
- R244, R241, R593, HF-1189SP-1, HF-1189SP
- Formula44, 285, 245, HF-1189CF, 1544-MIL and many more..

They all have a qual ref and a governm. Designation  like

R244 = QPL 14256-306-93 = ref M14256LRFP and so on.....

It's all called Kester's MIL-SPEC-BOOK for (water soluble) solder
formulas.

Most of them guarantee SIR uncleaned approx. 10exp11 Ohms and cleaned
10exp12 Ohms, which is well above most requirements.

You may put it this way: are the QPL'ed solders and fluxes what they
promise with regard to Cecilia's questions ? If they are, why bother?

Do you buy and apply QPL'ed solders/fluxes for your saucers? Or are you
a suspicious nature that doesn't accept anything before you have tested
the solders/fluxes yourself?

Kester is not favoured in this mail, was just an example. All other
solder/fluxe makers are supposed to have similar QPL'ed material.

/Ingemar



>         Hi Cecilia,
>  
> > I need some help on the following topic.
> > Is there any information available on using water soluble flux and
paste
> > in the military/defence industry?  
> >  
>         You can check IPC-HDBK-001 for general information on
soldering.
>         ANSI/J-STD-004 covers the requirements for soldering fluxes.
>         For the US Military, MIL-F-14256F, which was cancelled, covers
> fluxes.
>         ANSI/J-STD-001B covers the requirements for Soldered
Electrical
> Assemblies
>         For the US Military, MIL-STD-2000A, and MIL-S-45743E, both
cancelled
> without replacement, covered soldering).
>  
> > Does anyone have experience with this kind of flux system for
military
> > applications?
> >  
>         I haven't been around long but we are required to use what the
> customer specified in the original order which is usually RMA flux for
us.  
>  
> > How does the residues from water soluble flux affect the reliability
of
> > the product?
> >  
>         Others with more experience could give you a better picture of
> reliability issues.
>         Residues on the board shouldn't be ionic otherwise a short
could
> develop between pins/connectors over time.
>         Nonionic residues can be a trap for ionic ones. Our customers
don't
> like to see dirty boards and neither do we.
>  
>         Alot of Military products I've seen require the boards to be
> conformally coated and so the boards have to be clean very well after
> soldering.
>  
>         Hans
>  
> Air Force Material Command - We keep them flying!
> ~~~~~~~~
> Hans M. Hinners                                 WR-ALC/LYPME Bldg. 640
> Materials Engineer                                      380 Second
Street,
> Suite 104
> Manufacturing Eng. Sec.                         Robins AFB GA
31098-1638
> 912-926-1970 (Voice) 468 - 1970 (DSN)   912-926-7974 (Fax)
> [log in to unmask]
>  
>  
> > Cecilia Alkhagen
> > ******************************************
> > Ericsson Microwave Systems AB
> > Production Engineering Development
> > Bergfotsgatan 2
> > S-431 84 Mölndal
> >  
> > Telephone +46 31 747 0000
> > Direct       +46 31 747 0288
> > Fax          +46 31 747 2635
> >  
> > ##############################################################
> > TechNet Mail List provided as a free service by IPC using LISTSERV
1.8c
> > ##############################################################
> > To subscribe/unsubscribe, send a message to [log in to unmask] with
> > following text in
> > the body:
> > To subscribe:   SUBSCRIBE TECHNET <your full name>
> > To unsubscribe:   SIGNOFF TECHNET
> > ##############################################################
> > Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
> > additional
> > information.
> > If you need assistance - contact Gayatri Sardeshpande at
[log in to unmask] or
> > 847-509-9700 ext.5365
> > ##############################################################
>  
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV
1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
following text
>  in
> the body:
> To subscribe:   SUBSCRIBE TECHNET <your full name>
> To unsubscribe:   SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
> information.
> If you need assistance - contact Gayatri Sardeshpande at
[log in to unmask] or
> 847-509-9700 ext.5365
> ##############################################################
>  

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################

ATOM RSS1 RSS2