Hi Cecilia,
> I need some help on the following topic.
> Is there any information available on using water soluble flux and paste
> in the military/defence industry?
>
You can check IPC-HDBK-001 for general information on soldering.
ANSI/J-STD-004 covers the requirements for soldering fluxes.
For the US Military, MIL-F-14256F, which was cancelled, covers
fluxes.
ANSI/J-STD-001B covers the requirements for Soldered Electrical
Assemblies
For the US Military, MIL-STD-2000A, and MIL-S-45743E, both cancelled
without replacement, covered soldering).
> Does anyone have experience with this kind of flux system for military
> applications?
>
I haven't been around long but we are required to use what the
customer specified in the original order which is usually RMA flux for us.
> How does the residues from water soluble flux affect the reliability of
> the product?
>
Others with more experience could give you a better picture of
reliability issues.
Residues on the board shouldn't be ionic otherwise a short could
develop between pins/connectors over time.
Nonionic residues can be a trap for ionic ones. Our customers don't
like to see dirty boards and neither do we.
Alot of Military products I've seen require the boards to be
conformally coated and so the boards have to be clean very well after
soldering.
Hans
Air Force Material Command - We keep them flying!
~~~~~~~~
Hans M. Hinners WR-ALC/LYPME Bldg. 640
Materials Engineer 380 Second Street,
Suite 104
Manufacturing Eng. Sec. Robins AFB GA 31098-1638
912-926-1970 (Voice) 468 - 1970 (DSN) 912-926-7974 (Fax)
[log in to unmask]
> Cecilia Alkhagen
> ******************************************
> Ericsson Microwave Systems AB
> Production Engineering Development
> Bergfotsgatan 2
> S-431 84 Mölndal
>
> Telephone +46 31 747 0000
> Direct +46 31 747 0288
> Fax +46 31 747 2635
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in
> the body:
> To subscribe: SUBSCRIBE TECHNET <your full name>
> To unsubscribe: SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
> additional
> information.
> If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
> 847-509-9700 ext.5365
> ##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|