Well ' we're getting there :
1
Yes ; the round balls 8x smaller go better through needle than 2x only
smaller flakes
But that obviously does not matter , as well as the tip temperatures as you
just removed it and it's still clogging !
Inge , perhaps last desperate idea :
You said the flakes are 1-50um .
reading the tolerances would give logical conclusion the flakes can build up
between the wall and outer auger surface.
Can you describe the clog : deposition on ceramic wall, inside the auger
groove , or a plug on exit ?
Sounds (wild idea) like the flakes could be smudged on wall ; compressed to
super flakes and jam eventually .
Is there a grade like 25-50um (bit wishful, I know)?
Shaafi worked with 642 for a decade+ ; see if he can help .
Shaafi, could you please help us to resolve this mystery ?
Subject is silver loaded epoxy clogging WITHOUT NEEDLE .
Seen anything like this ?
Inge's climbing walls and us the netters don't like to give up .
Thanks a lot ahead buddy .
If you'd be stuck too ; could you point us to somebody more experienced
still ?
I'd love to know myself ; this next lead-free millenium ain't going to be
fun .
What do you think about the 2psi ?
paul
-----Original Message-----
From: [log in to unmask]
[mailto:[log in to unmask]]
Sent: Monday, 16 August 1999 20:01
To: [log in to unmask]
Subject: Re: [TN] clogging dispensers
To you all that help me with finding reasons for clogging: pump is
Camelot 642-1, carbide housing and auger with following data
- thread depth is 85microns
- thread pitch is 1,500 microns
- thread peripherical is polished to Ra 40nm /TIR 300 nm
- thread shallow part is polished to Ra 1.5um/TIR 7um
- pressure at syringe level is 2 psi.
Needle removed: still clogging in the pump! Ain't she sweet! Don't know
if Tim wanted to be on his own. Some people do not want to cry out
details worldwide.
/Ingemar
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|