"Mengers, William D." <[log in to unmask]>
Date:
Mon, 16 Aug 1999 10:08:05 -0400
MIME-Version:
1.0
X-To:
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, "Mengers, William D." <[log in to unmask]>
Parts/Attachments:
text/plain (444 lines)
Scott,

I have done quite a bit of experimentation with an Asymtek dispenser using
thermocouples at various locations including the dispensing tip.  I had a
thermocouple on the end of a stiff wire and merely taped the wire to the
pump valve, leaving some spring in the wire and letting it rest against the
tip in some thermal grease to make sure there was good heat transfer between
the tip and the thermocouple.  It worked fine.  If we wanted to change tips
we could do it anytime and as frequent as desired just by moving the wire
slightly.  Hope this helps.

Bill Mengers
Northrop Grumman
Process Engineer

        -----Original Message-----
        From:   [log in to unmask]
[SMTP:[log in to unmask]]
        Sent:   Monday, August 16, 1999 9:54 AM
        To:     [log in to unmask]
        Subject:        Re: [TN] clogging dispensers

        Scott,
        as we have some laser welding equipments, it could be worth a cent
to
        weld a micro thermal couple to the tip. Multicore's oven temp check
box
        for PC may work as data aquisitor. We have successfully welded such
        miniwires on inside of MCMs for monitoring temperature in different
        places during laser seam welding. / Ingemar


        > Ingemar,
        >
        > We attempted to attach a thermal couple to the tip and then hook
the
        thermal
        > couple up to a data logger so we could plot the temperature over
time.
        > Unfortunately the thermal couple wouldn't stay attached to the tip
of
        the
        > glue nozzle even though we tried every epoxy and tape in our
arsenal.
        >
        > As Paul eluded to in a previous post, the tips did not touch the
board
        but
        > the stand-off did.
        >
        > Scott
        > -----Original Message-----
        > From: [log in to unmask]
        > [mailto:[log in to unmask]]
        > Sent: Monday, August 16, 1999 2:47 AM
        > To: [log in to unmask]
        > Subject: Re: [TN] clogging dispensers
        >
        >
        > Dear Paul&Jason (sounds like a rock group),
        > your openminded support and will to do something is something.
Now,
        > gage vs. syringe will be under observance, so will your experience
        about
        > hardrunning still without heat build-up. The one who told about
it:
        did
        > you guess or did you in fact measure the tip's heat? Don't grasp
what
        > you mean with 'simple' men, suspect some sort of double-edge
        paraphrase.
        > Your thumb rule 8xflaw size is good. Our auger has a trapetsoid
        thread,
        > outer circumference polished, space in between very rough indeed,
you
        > say this roughness doesn't matter, thought opposite. Mentioned
silver
        > filled polymer not same problems as with lead/tin ditos, then
what's
        the
        > difference: (corn) flakes vs. balls? Are balls less benign to
clogging
        > than flakes?
        > See you on the CRT glass
        > Ingemar Hernefjord
        > Ericsson Microwave Systems
        >
        >
        > > Jason,
        > > once you'll go over 24 gauge (25, 26) ; you'll need 400-500 mesh
;
        > > we use indium nc-smq90 in 200 gms cartridges ; on 644 head ;
        > > 2x 200 on back (2x 50 on front) .
        > > eventually (after a year we found the mesh price difference did
        > justify the
        > > yields ; about 1-2 blocked needles a week with nonstop three
shifts)
        > we
        > > dropped the 325 all together ;
        > > dispensing 400-500 only across all gauges .
        > > The pressure running up to auger is 25 psi (on 200 cartridge);
10
        (on
        > 50
        > > cartridge).
        > > We run second year on it ; it's proven , no problems ; ask
indium
        guys
        > for
        > > 200gr ResMed's package and give it a shot (you need to make
yourself
        > custom
        > > clamp ; to counter the G's generated)
        > >
        > > And > Inge did cry about silver loaded polymer, not solder/flux
        paste:
        > not
        > > quite the same .
        > >
        > > Scott,
        > > never experienced the increased temps even after 8 hour
literally
        non
        > stop ;
        > > on Gemini's validations all went in (paste, silver, glue,
thermal
        > transfer
        > > compounds) ;
        > > and the needle never touches the board (the foot does) .
        > >
        > > Tim decided to stay incognito ; which is a pity ; not what the
net
        is
        > about
        > > .
        > >
        > > So finally , dear nett(?)er Inge :
        > > When you look onto those suspended silver particles under your
        trusted
        > scope
        > > ;
        > > you find that those ain't particularly balls (camelot says for
        example
        > the
        > > inner needle dia should be minimum of 8x the ball [solder]size)
        > > I particularly do not think you need a rocket; morphology; fluid
        > dyno's;
        > > rheologies and polishing compounds and tolerancing sciences to
give
        > you a
        > > hint you're applying wrong needle gauge for the job . The
auger's
        side
        > walls
        > > (twiddling in ceramic shaft I presume) are precision ground ;
the
        > inner of
        > > needles is good enough .
        > > By the sound of it you just started this applications ;
therefore
        you
        > have
        > > in front of you a lot of trials and validations, and the simple
men
        > from
        > > manufacturer (not paste supplier) would do you good as they did
        > (should) a
        > > lot of it .
        > >
        > > Being simple man myself ; I'd (perhaps naively) presume to push
down
        > up to
        > > 50(!)um silver boulders through 100(!)um inner orifice may cause
you
        a
        > > mighty pain :
        > > this being caused by sheer wishful thinking .
        > >
        > > Familiar indeed
        > >
        > > Anyhow, wish you luck ; keep in touch if you're still stuck ;
        > > and let me know what you thought (don't hold back ; I can take
it)
        > about my
        > > reflection on the thermal transfer = how did your bubbles go ???
        > > Werner said he prefers steaks to snitzels ; and I have to admit
I
        > always saw
        > > the breadcrumbs "extension" as poor culinary pretences .
        > > Sorry Norman , done now
        > >
        > >
        > > Paul Klasek
        > > http://www.resmed.com
        > >
        > >
        > >
        > >
        > >
        > >
        > >
        > >
        > >
        > >
        > >
        > >
        > >
        > > -----Original Message-----
        > > From: jason gregory [mailto:[log in to unmask]]
        > > Sent: Saturday, 14 August 1999 0:20
        > > To: [log in to unmask]
        > > Subject: Re: [TN] clogging dispensers
        > >
        > >
        > > I had the same problem and addressed it on the smtnet.com site.
I
        was
        > using
        > > a paste mesh that is suitable for screening, not dispensing
(325/500
        > mesh).
        > > I figured the only bad thing that would occur would be that the
        paste
        > > wouldn't flow as easily through my nozzle. After purging the
pump to
        > remove
        > > all air bubbles, the flow would stop and I would disassemble the
        pump
        > and
        > > find a hard, shiny chunk of solder at the end of the pump,
before
        the
        > > nozzle, impeding the flow, that appeared reflowed. My guess,
coupled
        > with
        > > knowledgeable persons agreeing, was that the mesh indicates a
larger
        > ball
        > > size and the "resistance" of the balls to flow through the
nozzle
        was
        > > causing great friction inside the pump, compounding the balls
        together
        > and
        > > possibly the constant friction was causing the backing-up solder
to,
        > in
        > > essence, "flow". Check your paste mesh. BTW, I am using a
Camalot
        5000
        > with
        > > an Archimedes-style pump. Hope some of this helps.
        > >
        > > > -----Original Message-----
        > > > From: [log in to unmask]
        > > > [SMTP:[log in to unmask]]
        > > > Sent: Friday, August 13, 1999 8:41 AM
        > > > To:   [log in to unmask]
        > > > Subject:      [TN] clogging dispensers
        > > >
        > > > Out of 1,700 netters, someone should have an idea about this:
        > > >
        > > > We need expertise advice immediately to solve a mystery with
        > clogging
        > > > high speed automatic dispensers. Three silver epoxy pastes
give
        same
        > > > clogging. Fresh pastes are bought. Same. Dispenser screws,
tubes,
        > pumps,
        > > > all details are cleaned thoroughly. Same. New dispenser parts
        > installed.
        > > > Same. Whatever we do. Same. After running some minutes-hours:
        > clogging
        > > > in the needle. Some say that the room humidity must be very
exact
        in
        > > > order to make the dispenser epedize well. Others talk about
local
        > curing
        > > > inside the paste. And some think sedimentation can be the
plague.
        > > > Experts from the paste manufacturer will be here in one or two
        days,
        > but
        > > > according to my experience, they seldom have that kind of
knowhow,
        > > > machine makers can have, this one not. Most oftenly, the
        knowhowers
        > are
        > > > people like you, dear nett(l)ers.
        > > >
        > > > I have my own theory, but can't prove it yet. Namely, that
this
        > > > "conglomerate" or mix of fluids and silver flaws (1-50um) can
be
        > > > PRESSURE DEPENDENT, i.e. at certain constant or momentary
        pressure,
        > > > there will be a separation in the narrowest part, the needle,
        fluids
        > > > will drop out and separate, leaving the coarser silver flaws
        without
        > > > fluency, they will clog. Also, I have seen that the inside of
the
        > needle
        > > > (inner dia 100um) is not polished, but has a rather grainy
        stucture,
        > > > likwise the rotating helix that feeds paste. Both should be
        > polished, I
        > > > suppose. There is a science that use morphology and fluiding
        > dynamics
        > > > that possibly can give a clue, but I'm rather far from that
art,
        > maybe
        > > > some of you have education of the sort.
        > > >
        > > > Familiar to someone?
        > > >
        > > > Remo@Alenia, if you read this, please contact me, I have lost
your
        > > > adress.
        > > >
        > > > Thanks in advance/
        > > > Ingemar Hernefjord
        > > > Ericsson Microwaves Systems
        > > >
        > > > ##############################################################
        > > > TechNet Mail List provided as a free service by IPC using
LISTSERV
        > 1.8c
        > > > ##############################################################
        > > > To subscribe/unsubscribe, send a message to [log in to unmask]
with
        > > > following text in
        > > > the body:
        > > > To subscribe:   SUBSCRIBE TECHNET <your full name>
        > > > To unsubscribe:   SIGNOFF TECHNET
        > > > ##############################################################
        > > > Please visit IPC web site (http://www.ipc.org/html/forum.htm)
for
        > > > additional
        > > > information.
        > > > If you need assistance - contact Gayatri Sardeshpande at
        > [log in to unmask] or
        > > > 847-509-9700 ext.5365
        > > > ##############################################################
        > >
        > > ##############################################################
        > > TechNet Mail List provided as a free service by IPC using
LISTSERV
        > 1.8c
        > > ##############################################################
        > > To subscribe/unsubscribe, send a message to [log in to unmask]
with
        > following
        > > text in
        > > the body:
        > > To subscribe:   SUBSCRIBE TECHNET <your full name>
        > > To unsubscribe:   SIGNOFF TECHNET
        > > ##############################################################
        > > Please visit IPC web site (http://www.ipc.org/html/forum.htm)
for
        > additional
        > > information.
        > > If you need assistance - contact Gayatri Sardeshpande at
        > [log in to unmask] or
        > > 847-509-9700 ext.5365
        > > ##############################################################
        > >
        > > ##############################################################
        > > TechNet Mail List provided as a free service by IPC using
LISTSERV
        > 1.8c
        > > ##############################################################
        > > To subscribe/unsubscribe, send a message to [log in to unmask]
with
        > following text
        > >  in
        > > the body:
        > > To subscribe:   SUBSCRIBE TECHNET <your full name>
        > > To unsubscribe:   SIGNOFF TECHNET
        > > ##############################################################
        > > Please visit IPC web site (http://www.ipc.org/html/forum.htm)
for
        > additional
        > > information.
        > > If you need assistance - contact Gayatri Sardeshpande at
        > [log in to unmask] or
        > > 847-509-9700 ext.5365
        > > ##############################################################
        > >
        >
        > ##############################################################
        > TechNet Mail List provided as a free service by IPC using LISTSERV
        1.8c
        > ##############################################################
        > To subscribe/unsubscribe, send a message to [log in to unmask] with
        following
        > text in
        > the body:
        > To subscribe:   SUBSCRIBE TECHNET <your full name>
        > To unsubscribe:   SIGNOFF TECHNET
        > ##############################################################
        > Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
        additional
        > information.
        > If you need assistance - contact Gayatri Sardeshpande at
        [log in to unmask] or
        > 847-509-9700 ext.5365
        > ##############################################################
        >

        ##############################################################
        TechNet Mail List provided as a free service by IPC using LISTSERV
1.8c
        ##############################################################
        To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in
        the body:
        To subscribe:   SUBSCRIBE TECHNET <your full name>
        To unsubscribe:   SIGNOFF TECHNET
        ##############################################################
        Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
        information.
        If you need assistance - contact Gayatri Sardeshpande at
[log in to unmask] or
        847-509-9700 ext.5365
        ##############################################################

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or