Hello Technetters,
We are doing a job of soldering around 4500 pins into a Glass Epoxy
Multilayer PCB of size 288 x 200 mm. The pins are first push fit into the
PCB . The pins protrude on both sides of the PCB . On once side the pins
will mate with a connector, and on the other side wires are wrapped on. 1
Solder ring ( 0.9 mm dia ) is then put over each pin . The board is then put
in a reflow over for 180 sec at 235 deg C. We find that the solder joint are
not properly formed, and the finish is quite dull. The solder ring is
composed of 62% Tin, 2 % Silver, 34 % Lead. The solder flows out to the
other side of the PCB , but is not quite enough. We also notice
discoloration of the PCB after this cycle.
What are the issues that we need to be looking at here, to get a better
joint with a better finish . We are completely new to this .
Appreciate some inputs and tips on doing this
With warm regards
Deepak Kuriyan
Framatome Connectors OEN
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|