TECHNET Archives

February 1998

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Transfer-Encoding:
7bit
Sender:
Subject:
From:
Gabriela Bogdan <[log in to unmask]>
Date:
Mon, 2 Feb 1998 09:05:54 +0000
Content-Type:
text/plain; charset=us-ascii
MIME-Version:
1.0
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Gabriela Bogdan <[log in to unmask]>
Parts/Attachments:
text/plain (34 lines)
Dear TechNetters !
Assuming that the boards are ordered and manufactured according to
IPC-J-STD-003,but stored in a noncontrolled environment for more
than 1 year, I would like help on the  following-(for eutectic
tin/lead):
1.What is the known growth rate of the intermetallic,and what is the
minimum tin/lead thickness left?
2.If there is moisture absorbed,but the plating in holes is without
defects
concerning thickness,voids,drilling,a.s.o.,should I expect blowholes?
3.What is the maximum intermetallic growth after drying for 3 hrs at
120C?
4.Are delamination problems encountered in almost all or few boards
which absorbed moisture ,and is this related more to the manufacturer's
workmanship?
5.Finally would drying decrease solderability so much as to render
boards
unsolderable with no-clean fluxes?
Could somebody give me some information very QUICKLY?
Thank you all,
GABY

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################


ATOM RSS1 RSS2