Thermount is duPonts name for it's random Aramid fiber. It is used to make
boards where expansion in x and y are constrained. There are several
suppliers of laminate based on it that I am aware of Neltec for epoxy based,
and Arlon for polyimide based.
DuPont contacts are: David Powell 207-865-4090
[log in to unmask]
or Bill Allfather at 302-999-2250
Arlon is at 909-987-9533
Neltec is at 602-967-5600
----------
From: [log in to unmask]
To: [log in to unmask]
Subject: Fab - material
Date: Friday, April 18, 1997 10:10AM
Could someone point me in the right direction to get
information on Thermount material.
Thankyou
Don Bloye
PC World
[log in to unmask]
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]> *
* with <subject: subscribe/unsubscribe> and no text in the body. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]> *
* with <subject: subscribe/unsubscribe> and no text in the body. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************