Thermount is duPonts name for it's random Aramid fiber. It is used to make boards where expansion in x and y are constrained. There are several suppliers of laminate based on it that I am aware of Neltec for epoxy based, and Arlon for polyimide based. DuPont contacts are: David Powell 207-865-4090 [log in to unmask] or Bill Allfather at 302-999-2250 Arlon is at 909-987-9533 Neltec is at 602-967-5600 ---------- From: [log in to unmask] To: [log in to unmask] Subject: Fab - material Date: Friday, April 18, 1997 10:10AM Could someone point me in the right direction to get information on Thermount material. Thankyou Don Bloye PC World [log in to unmask] *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To subscribe/unsubscribe send a message <to: [log in to unmask]> * * with <subject: subscribe/unsubscribe> and no text in the body. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * *************************************************************************** *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To subscribe/unsubscribe send a message <to: [log in to unmask]> * * with <subject: subscribe/unsubscribe> and no text in the body. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * ***************************************************************************