TECHNET Archives

April 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
X400-Content-Type:
P2-1988 ( 22 )
From [log in to unmask] Fri Apr 18 11:
30:07 1997
Date:
18 Apr 1997 11:22:30 -0500
X-Loop:
Precedence:
list
Resent-From:
Conversion:
Allowed
Disclose-Recipients:
Prohibited
Resent-Sender:
TechNet-request [log in to unmask]
X-Status:
Status:
O
Priority:
normal
X-Mailing-List:
<[log in to unmask]> archive/latest/12118
X400-Originator:
Content-Return:
Allowed
X400-MTS-Identifier:
[/c=US/admd=MCI/prmd=Honeywell/; 0638933579FC61E0-HW-MTA-AZ]
TO:
"[log in to unmask]" <[log in to unmask]> (Return requested)
Received:
by ipc.org (Smail3.1.28.1 #2) id m0wIGKt-000Bj8C; Fri, 18 Apr 97 11:16 CDT
Return-Path:
<TechNet-request>
cc:
"[log in to unmask]" <[log in to unmask]> (Return requested)
X400-Recipients:
non-disclosure;
Alternate-Recipient:
Allowed
Message-Id:
<0638933579FC61E0*/c=US/admd=MCI/prmd=Honeywell/o=AZ-MTA/ou=MSMail/ou=CAS/s=Edwards/g=Ted/i=A/@MHS>
Resent-Message-ID:
<"-X0CR.0.3KO.RvvLp"@ipc>
Subject:
From:
"Edwards, Ted A (AZ75)" <[log in to unmask]>
Old-Return-Path:
X400-Received:
by mta HW-MTA-AZ in /c=US/admd=MCI/prmd=Honeywell/; Relayed; 18 Apr 1997 11:22:30 -0500 by /c=US/admd=MCI/prmd=Honeywell/; Relayed; 18 Apr 1997 11:22:30 -0500
Original-Encoded-Information-Types:
IA5-Text
Content-Identifier:
0638933579FC61E0
Parts/Attachments:
text/plain (48 lines)
Thermount is duPonts name for it's random Aramid fiber.  It is used to make 
boards where expansion in x and y are constrained.  There are several 
suppliers of laminate based on it that I am aware of Neltec for epoxy based, 
and Arlon for polyimide based.
     DuPont contacts are:  David Powell 207-865-4090
[log in to unmask]

     or Bill Allfather at 302-999-2250

     Arlon is at 909-987-9533

     Neltec is at 602-967-5600

 ----------
From: [log in to unmask]
To: [log in to unmask]
Subject: Fab - material
Date: Friday, April 18, 1997 10:10AM

     Could someone point me in the right direction to get
     information on Thermount material.
        Thankyou
        Don Bloye
     PC World
        [log in to unmask]

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************



ATOM RSS1 RSS2