No organic coating will completely seal out moisture. That said,
IPC-CC-830 is the industry standard for conformal coatings. To obtain a
copy, call IPC's order department at 847-509-9700, ext. 316.
Mike Buetow
IPC Staff
2215 Sanders Road
Northbrook, IL 60062
P: 847-509-9700, ext. 335
F: 847-509-9798
[log in to unmask]
On Thu, 27 Mar 1997, William Johnson wrote:
> Is there a commercial procedure available for coating printed circuit boards
> to prevent corrosion caused by the salt water mist that sometimes permeates a
> boat?
>
> ***************************************************************************
> * TechNet mail list is provided as a service by IPC using SmartList v3.05 *
> ***************************************************************************
> * To subscribe/unsubscribe send a message <to: [log in to unmask]> *
> * with <subject: subscribe/unsubscribe> and no text in the body. *
> ***************************************************************************
> * If you are having a problem with the IPC TechNet forum please contact *
> * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
> ***************************************************************************
>
>
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]> *
* with <subject: subscribe/unsubscribe> and no text in the body. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
|
|
|