No organic coating will completely seal out moisture. That said, IPC-CC-830 is the industry standard for conformal coatings. To obtain a copy, call IPC's order department at 847-509-9700, ext. 316. Mike Buetow IPC Staff 2215 Sanders Road Northbrook, IL 60062 P: 847-509-9700, ext. 335 F: 847-509-9798 [log in to unmask] On Thu, 27 Mar 1997, William Johnson wrote: > Is there a commercial procedure available for coating printed circuit boards > to prevent corrosion caused by the salt water mist that sometimes permeates a > boat? > > *************************************************************************** > * TechNet mail list is provided as a service by IPC using SmartList v3.05 * > *************************************************************************** > * To subscribe/unsubscribe send a message <to: [log in to unmask]> * > * with <subject: subscribe/unsubscribe> and no text in the body. * > *************************************************************************** > * If you are having a problem with the IPC TechNet forum please contact * > * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * > *************************************************************************** > > *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To subscribe/unsubscribe send a message <to: [log in to unmask]> * * with <subject: subscribe/unsubscribe> and no text in the body. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * ***************************************************************************