No organic coating will completely seal out moisture. That said, 
IPC-CC-830 is the industry standard for conformal coatings. To obtain a 
copy, call IPC's order department at 847-509-9700, ext. 316.

Mike Buetow
IPC Staff
2215 Sanders Road
Northbrook, IL 60062
P: 847-509-9700, ext. 335
F: 847-509-9798
[log in to unmask]


On Thu, 27 Mar 1997, William Johnson wrote:

> Is there a commercial procedure available for coating printed circuit boards 
> to prevent corrosion caused by the salt water mist that sometimes permeates a 
> boat?
> 
> ***************************************************************************
> * TechNet mail list is provided as a service by IPC using SmartList v3.05 *
> ***************************************************************************
> * To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
> * with <subject: subscribe/unsubscribe> and no text in the body.          *
> ***************************************************************************
> * If you are having a problem with the IPC TechNet forum please contact   *
> * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
> ***************************************************************************
> 
> 

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************



ATOM RSS1 RSS2