Received: |
by ipc.org (Smail3.1.28.1 #2)
id m0va9qn-0000GTC; Tue, 17 Dec 96 18:27 CST |
Content-Type: |
TEXT/PLAIN; CHARSET=ISO-8859-1 |
Old-Return-Path: |
|
Date: |
Tue, 17 Dec 1996 19:15:39 -0500 |
Precedence: |
list |
Resent-From: |
|
Resent-Sender: |
|
MIME-Version: |
1.0 (WebTV 1.0) |
Status: |
O |
X-Mailing-List: |
|
TO: |
|
Return-Path: |
<TechNet-request> |
X-Status: |
|
Resent-Message-ID: |
<"mRVMG3.0.xwB.Sfpjo"@ipc> |
Subject: |
|
From: |
|
X-Loop: |
|
From [log in to unmask] Wed Dec 18 08: |
23:27 1996 |
Content-Transfer-Encoding: |
QUOTED-PRINTABLE |
Message-Id: |
|
Parts/Attachments: |
|
|
Technet!
Our quartz cooling jackets for double sided UV curing lamps generate
2000W of energy and much heat.
The quartz jackets become striated and stressed at the fused ends. Also
material adheres to the inner wall closest to the lamp over time.
1) Does anyone know what this material coating is? (We use distilled
water in the cooling jacket and two hoses connected inside the unit.)
and 2) Would a routine annealing remove the material and / or
stress?
Thank yinz ahead of time.
P.G. Wilson
[log in to unmask]
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to: *
* [log in to unmask] with <subject: unsubscribe> and no text. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
|
|
|