NASA uses NHB 5300.4(3G) "Requirements for interconnecting cables
harnesses, and wiring"
There is also mil-std-2000 (which may, or may not be released)
for "soldering electrical and electronic assemblies"
Also Mil-std-454 "Standard general req. for electronic equipment"
These are the customer specs that I have to go by.
Bill Gaines
AeroJet (for $) 1100 Hollyvale, Azusa, Calif. 91702-0298
IEPS (for info) [log in to unmask]
IHPVA (for speed & fun) P.O. Box 51255, IN, IN 46251-0255
SCCA (for trophys) Solo II (818-988-RACE)===================================================