Good morning Rich,
We have used the following with good success.
Kester Wondermask P - heat curable
Dymax Emax 906B and Dymax 9-20515 - UV curable masks. The 906B is blue and
thicker. The other is red and thinner.
Loctite AS8998 hot melt masking agent.
---
*Douglas Pauls *| Principal Materials and Process Engr | Advanced
Operations Engineering
*COLLINS AEROSPACE*
400 Collins Road NE, MS 108-101, Cedar Rapids, IA 52498 USA
*Tel:* +1 319 295 2109 | *Mobile: *+1 319 431 3773
[log in to unmask]
[log in to unmask] for all Export Compliant Items
On Fri, Jan 8, 2021 at 8:53 AM Richard Kraszewski <
[log in to unmask]> wrote:
> Our preferred "non-ammoniated" liquid masking material for coating is on
> back order.
> I need to find another product.
> Can anyone please share which masking they have good success with?
>
> Rich Kraszewski
> Senior Staff Process Engineer
> Phone: (920) 969-6075
>
> * * * * * * * * CONFIDENTIALITY NOTICE * * * * * * * *
> This e-mail and any attachments are confidential from Plexus Corp. and may
> contain information which is privileged, confidential, and/or protected by
> non-disclosure agreements. They are intended solely for the use of the
> named addressee(s). . Any unauthorized use or disclosure may be
> unlawful. If you are not a named addressee, you must not use, disclose,
> retain or reproduce all or any part of the information contained in this
> e-mail or any attachments If you have received this transmission in error,
> please destroy it and notify us immediately by return e-mail or by calling
> + 1 888 208 9005.
>
|
|
|