TECHNET Archives

June 2011

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
GRIVON Arnaud <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, GRIVON Arnaud <[log in to unmask]>
Date:
Wed, 29 Jun 2011 17:19:47 +0200
Content-Type:
text/plain
Parts/Attachments:
text/plain (64 lines)
TechNetters,

It looks like my earlier query on the best practice to use for strapping two adjacent vias at the bottom of a BGA has been partcularly unsuccessful with no reply so far, which is quite unusual for the TechNet forum...
This message is only a reminder or a second chance...
Thanks for sharing your views on this topic.
Best regards, 

Arnaud Grivon
PCB/PCBA Technology Expert
Thales Corporate Services - EPM
18, avenue du Maréchal Juin
Bât. C - Bureau C2-135
92366 Meudon-la-Forêt Cedex
France
Tél : (+33) (0)1 70 28 23 88

-----Message d'origine-----
De : TechNet [mailto:[log in to unmask]] De la part de GRIVON Arnaud
Envoyé : mercredi 22 juin 2011 17:46
À : [log in to unmask]
Objet : [TN] [COM] Strapping Adjacent BGA Vias

Dear all,

What would the best repair process to use for strapping two adjacent vias of a 1mm-pitch BGA?
I did not find this situation in the IPC-7711/7721 standard.
Soldering a jumper wire in the two vias at the BGA bottom side looks risky because of the possibility of partially reflowing the BGA joints, but this may not be a real concern for a small wire.
Soldering a chip could be another option, but I am not sure this is an acceptable practice.
Insights welcome. Assume worst case, i.e. requirements to ensure high-reliability and harsh environment.
Thanks in advance.

A. Grivon


______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2