Lee,
To the best of my knowledge, the definitive public information on the subject is from NPL. It's free from their website. See abstract below.
Chris
Chris Mahanna
Robisan Lab
Title:
XRF measurement of residual materials in electronics.
Author:
Wickham, M, Hunt, C
(An asterisk (*) after an author's name indicates a non-NPL author)
Source:
MAT 4, August 2007
ISSN: 1754-2979
Abstract:
The aim of this study was to assess the suitability of using X-ray fluorescence (XRF) systems for screening electronics parts in two applications - compliance with RoHS regulations, and tin whisker mitigation. Fifteen XRF systems were evaluated using typical electronic components and assemblies, ranging from contaminated plastic components, through bulk solder alloys, to solder joints and solder-terminated components. The results indicate that while PIN (semiconductor diode) and SiLi detector based systems are suitable for RoHS compliance measurements in plastics and solders, proportional counter based systems are not. XRF systems using PIN or SiLi detectors generally proved efficient at distinguishing between non-compliant components (containing typically 2000+ppm of restricted substances) and compliant components (typically <500ppm of restricted substances). For levels between 500ppm and 2000ppm, the use of additional techniques may be required to provide discrimination. The PIN or SiLi detectors also proved efficient at distinguishing compliant and noncompliant systems containing >1000ppm cadmium. Below this level, however, additional techniques may again be required to provide discrimination. The lower RoHS limit for cadmium of 100ppm did result in a number of false detections for this element. Proportional counter based systems were capable of registering the presence of RoHS-banned elements at levels >3% e.g. such as found in some plastics. Below this level, however, their ability to detect any banned substances was questionable, and their use for such applications is not recommended. For tin whisker mitigation applications, lead levels in excess of 4% are required for solder samples. All the systems successfully detected lead at or above this level, providing the sample size was large enough to fill the measurement window. Indeed, all systems proved capable of detecting/measuring lead levels above 1% in solder. It is important to remember that the use of these instruments for both the applications studied (RoHS compliance, or tin whisker mitigation) requires the operators to have both a thorough knowledge of the instrument themselves, and a good understanding of the structure and materials involved in the test samples These are required to prevent incorrect interpretation of the data provided i.e. incorrect indications of RoHS compliance, or of tin whisker mitigation (e.g. for samples having lead in base materials beneath a lead-free metalisation). Recommendations on instrument practice to obtain meaningful, repeatable results are given.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Lee Whiteman
Sent: Tuesday, December 15, 2009 9:40 AM
To: [log in to unmask]
Subject: Re: [TN] Lead Free Analyzers
If you google "Portable XRF Analyzers", you would find several.
Good luck.
Lee Whiteman, PMP
Senior Member Engineering Staff
L-3 Communications East
Telephone: (856) 338-3508
FAX: (856) 338-2906
E-Mail: [log in to unmask]
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Leland Woodall
Sent: Tuesday, December 15, 2009 8:42 AM
To: [log in to unmask]
Subject: [TN] Lead Free Analyzers
Folks,
Since we're on the subject of RoHS, can someone please recommend a good, accurate, handheld lead free analysis unit, and its approximate cost?
We have a SEM and an XRF, but was wondering if we might be able to identify something a bit more portable to use in areas besides the lab.
Thanks,
Leland
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|