OOps.
rough estimating? more like rough conversion, rough typing, rough day....
yes, there really is at least 8.2 microinches of gold on the board in some areas.
no, that doesn't "=" the solder paste thickness, which is 6 mils.
But the curiosity is still as indicated - maybe that thick gold was enough to
mask the grain of the nickel and make it look like hard gold, and I wonder how
much gold is ending up in that solder joint, and what problems I might have.
I'm probably reaching, but I don't know what it's going to take to convince
purchasing that cheap boards cost money. Is there something in such a
variable and thick gold surface that would help indicate a high reliability risk? I
think it's getting where I need to show them a black/white answer whether
these boareds will fail or not.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|