Thanks steve. it is leadfree.
Steve Gregory wrote:
> Hi Sowmya!
>
> I have your picture posted, it's at:
>
> http://stevezeva.homestead.com/files/Resistor_R8_not_sitting_on_pad.JPG
>
> It looks like it's "drawbridged". Is your solderpaste lead-free?
>
> Steve
>
> -----Original Message-----
> From: Stadem, Richard D. [mailto:[log in to unmask]]
> Sent: Tuesday, October 28, 2008 8:55 AM
> To: TechNet E-Mail Forum; [log in to unmask]
> Cc: Steve Gregory
> Subject: RE: [TN] Solder fillet
>
> Good morning, Sowmya
> The Technet forum strips any attachments. However, an esteemed
> participant in the forum will post pictures and provide a link to the
> pictures so we can all view it. His name is Steve Gregory and you can
> send your picture to him at [log in to unmask]
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of [log in to unmask]
> Sent: Tuesday, October 28, 2008 5:38 AM
> To: [log in to unmask]
> Subject: [TN] Solder fillet
>
> Experts,
>
> Pls find the attached photo. We have noticed a small gap in the
> soldering of smt resistor and this resulted in functional failure. what
> would be the causes? please advise.
>
> Thanks,
> Sowmya
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
> unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
> (re-start) delivery of Technet send e-mail to [log in to unmask]: SET
> Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
> posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
> archives of previous posts at: http://listserv.ipc.org/archives Please
> visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
> additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100 ext.2815
> -----------------------------------------------------
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------
>
>
>
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|