TECHNET Archives

October 2008

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Wed, 29 Oct 2008 11:51:00 -0000
Reply-To:
Subject:
From:
Mike Fenner <[log in to unmask]>
Content-Transfer-Encoding:
7bit
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (137 lines)
 
If the problem is only at that site and all other positions of that device
are OK then the first thing to check is placement, then print/stencil
quality of that aperture. Then move onto profile and so on.
Most people know that misplaced components will align on reflow, but there
are limits. Badly misplaced (where the component is more on one pad than
another) can effect heat transfer rates.  So if the component is
asymmetrically placed or tilted on placing you certainly can get
wetting/reflow on one termination before the other leading to drawbrdging.

Regards 

Mike Fenner 
Indium Corporation 

T: + 44 1908 580 400 
M: + 44 7810 526 317 
F: + 44 1908 580 411 
E: [log in to unmask] 
W: www.indium.com 
Pb-free: www.Pb-Free.com 

---------------------

Indium Corporation
Incorporated in New York, USA
Registered office: (Not for correspondence) 
77-97 Harpur Street, Bedford , UK
Registered number: fc16473


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of [log in to unmask]
Sent: Wednesday, October 29, 2008 3:33 AM
To: [log in to unmask]
Subject: Re: [TN] Solder fillet

Thanks steve. it is leadfree.

Steve Gregory wrote:
> Hi Sowmya!
>
> I have your picture posted, it's at:
>
> http://stevezeva.homestead.com/files/Resistor_R8_not_sitting_on_pad.JPG
>
> It looks like it's "drawbridged". Is your solderpaste lead-free?
>
> Steve
>
> -----Original Message-----
> From: Stadem, Richard D. [mailto:[log in to unmask]]
> Sent: Tuesday, October 28, 2008 8:55 AM
> To: TechNet E-Mail Forum; [log in to unmask]
> Cc: Steve Gregory
> Subject: RE: [TN] Solder fillet
>
> Good morning, Sowmya
> The Technet forum strips any attachments. However, an esteemed 
> participant in the forum will post pictures and provide a link to the 
> pictures so we can all view it. His name is Steve Gregory and you can 
> send your picture to him at [log in to unmask]
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of 
> [log in to unmask]
> Sent: Tuesday, October 28, 2008 5:38 AM
> To: [log in to unmask]
> Subject: [TN] Solder fillet
>
> Experts,
>
> Pls find the attached photo. We have noticed a small gap in the 
> soldering of smt resistor and this resulted in functional failure. 
> what would be the causes? please advise.
>
> Thanks,
> Sowmya
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0 To 
> unsubscribe, send a message to [log in to unmask] with following text in 
> the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt 
> or
> (re-start) delivery of Technet send e-mail to [log in to unmask]: SET 
> Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
> posts: send e-mail to [log in to unmask]: SET Technet Digest Search the 
> archives of previous posts at: http://listserv.ipc.org/archives Please 
> visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
> for additional information, or contact Keach Sasamori at 
> [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0 To 
> unsubscribe, send a message to [log in to unmask] with following text in 
> the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt 
> or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET 
> Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the 
> posts: send e-mail to [log in to unmask]: SET Technet Digest Search the 
> archives of previous posts at: http://listserv.ipc.org/archives Please 
> visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
> for additional information, or contact Keach Sasamori at 
> [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------
>
>
>   

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives Please visit IPC web
site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------


***This email, its content, and any files transmitted with it, are intended solely for the addressee(s) and may be legally privileged and/or confidential. If you are not the intended recipient, please contact the sender by return and delete the material from any computer. Any review, retransmission, dissemination, or other use of, or taking of any action in reliance upon this information by persons or entities other than the intended recipient is prohibited.

Messages sent via this medium may be subjected to delays, non-delivery, and unauthorized alteration. This email has been prepared using information believed by the author to be reliable and accurate, but Indium Corporation makes no warranty as to accuracy or completeness. Indium Corporation does not accept responsibility for changes made to this email after is was sent. Any opinions or recommendations expressed herein are solely those of the author. They may be subject to change without notice.***

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2