TECHNET Archives

October 2008

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Steve Gregory <[log in to unmask]>
Date:
Tue, 28 Oct 2008 10:45:34 -0400
Reply-To:
Content-Transfer-Encoding:
7bit
Subject:
From:
Robert Kondner <[log in to unmask]>
Content-Type:
text/plain; charset="us-ascii"
In-Reply-To:
Organization:
Index Designs
MIME-Version:
1.0
Parts/Attachments:
text/plain (176 lines)
Hi,

 

  I am a newbie sitting on this list. I don't know if it would help but I do
have software which allows a user to look at how component metal fits over
pads and paste. It is free software, free as in "Free Beer".

 

Contact me   bob at Kondner dot com and I can get you a link. Picture below.

 

  I have a large number of part models but it is a pain learning how to use.


 

Bob Kondner

410-821-1315

 

RED = Component Model Metal. BLUE = solder paste

 



 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory
Sent: Tuesday, October 28, 2008 10:32 AM
To: [log in to unmask]
Subject: Re: [TN] Solder fillet

 

Hi Sowmya!

 

I have your picture posted, it's at:

 

http://stevezeva.homestead.com/files/Resistor_R8_not_sitting_on_pad.JPG

 

It looks like it's "drawbridged". Is your solderpaste lead-free?

 

Steve

 

-----Original Message-----

From: Stadem, Richard D. [mailto:[log in to unmask]] 

Sent: Tuesday, October 28, 2008 8:55 AM

To: TechNet E-Mail Forum; [log in to unmask]

Cc: Steve Gregory

Subject: RE: [TN] Solder fillet

 

Good morning, Sowmya

The Technet forum strips any attachments. However, an esteemed

participant in the forum will post pictures and provide a link to the

pictures so we can all view it. His name is Steve Gregory and you can

send your picture to him at [log in to unmask] 

 

-----Original Message-----

From: TechNet [mailto:[log in to unmask]] On Behalf Of [log in to unmask]

Sent: Tuesday, October 28, 2008 5:38 AM

To: [log in to unmask]

Subject: [TN] Solder fillet

 

Experts,

 

Pls find the attached photo. We have noticed a small gap in the

soldering of smt resistor and this resulted in functional failure. what

would be the causes? please advise.

 

Thanks,

Sowmya

 

---------------------------------------------------

Technet Mail List provided as a service by IPC using LISTSERV 15.0 To

unsubscribe, send a message to [log in to unmask] with following text in

the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or

(re-start) delivery of Technet send e-mail to [log in to unmask]: SET

Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the

posts: send e-mail to [log in to unmask]: SET Technet Digest Search the

archives of previous posts at: http://listserv.ipc.org/archives Please

visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for

additional information, or contact Keach Sasamori at [log in to unmask] or

847-615-7100 ext.2815

-----------------------------------------------------

 

---------------------------------------------------

Technet Mail List provided as a service by IPC using LISTSERV 15.0

To unsubscribe, send a message to [log in to unmask] with following text in

the BODY (NOT the subject field): SIGNOFF Technet

To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)

To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest

Search the archives of previous posts at: http://listserv.ipc.org/archives

Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815

-----------------------------------------------------


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2