TECHNET Archives

November 2007

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0 (Apple Message framework v752.3)
Sender:
X-To:
Date:
Thu, 1 Nov 2007 11:57:57 +0000
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Graham Naisbitt <[log in to unmask]>
Subject:
From:
Graham Naisbitt <[log in to unmask]>
X-cc:
In-Reply-To:
<007c01c81bee$95c91990$bc01a8c0@acerc28991bd48>
Content-Type:
multipart/mixed; boundary=Apple-Mail-23-862713250
Parts/Attachments:
text/plain (4 kB) , text/plain (6 kB)
Guy et al

Please do not confuse soldering ability with solderability. This was  
a subject covered by Dave Hillman some time ago but its worth  
repeating his words:

“The JSTD-002/003 solderability test standard's purpose is to test  
the robustness of a finish for wettability. Too many people attempt  
to use and/or believe that the standards are designed to mimic  
production conditions, they are not. This would be ‘soldering- 
ability’ not “solderability”.

Although the IPC committee has attempted to have the standards  
reflect soldering-ability concerns, it is not possible or practical  
in terms of testing methodology to mimic production. There are so  
many flux/process combination that the standards would cease to be of  
value; they would be huge and contain a multitude of variations.

The test parameters contained in the standards are designed to have  
some safety margin in terms of demonstrating the solderability of a  
surface - a test which gives either a false positive or false  
negative result is not of value to the industry.”

Now then, Sue asked about the flux used in the test and why it was  
changed.

We, in the committee, were faced with the need to develop the  
solderability test standards for the benefit of an industry facing  
the need to go lead-free. Consequently, and applying due diligence to  
the exercise, our Chairman and the committee felt it would be better  
to carry out a RR test programme examining the alloy, flux,  
temperature, and surface finishes that should be employed and to find  
Gauge R&R for the various methods used in the test.

This was a far better programme of work than the seemingly arbitrary  
International Standard from IEC - and I am the leader of that!

The testing extended to over 30,000 tests conducted at 6 different  
sites and statistically examined by the Guru Bill Russell (he's  
fluent in Swahili by the way!) No-one got paid for this, it was done  
for the benefit of the industry.

As regards the fluxes, SMNA and Actiec 2 and 5 have been proprietary  
grade materials and are my formulations when I bought the Multicore  
SPCID business from Henkel in 2002. IPC wanted to have access to  
these fluxes from other sources.

The flux for tin/lead solderability tests shall be a standard   
activated rosin flux #1 having a composition of 25% ± 0.5% by weight  
of colophony and 0.15% ± 0.01% by weight diethylammonium  
hydrochloride (CAS 660-68-4), in 74.85% ± 0.5% by weight of isopropyl  
alcohol. This is my Actiec 2

The flux for lead-free solderability tests shall be standard  
activated rosin flux #2 having a composition of  25% ± 0.5% by weight  
of colophony and 0.39% ± 0.01% by weight diethylammonium  
hydrochloride (CAS 660-68-4), in 74.61% ± 0.5% by weight of isopropyl  
alcohol. This is my Actiec 5

Keep in mind that the flux should be fresh for every test batch.

Can you use solderability testing to monitor your process - yes. Use  
the alloy, flux, temperature and surface finish on your process line  
and go right ahead. Just don't expect to control your suppliers that  
way as you will get false positives and false negatives.

I hope this helps and please, Richard, ease off on us folks who give  
out time free of charge to helping you all make better quality products.

Kindest regards
Graham Naisbitt

[log in to unmask]

www.gen3systems.com

Phone: +44 (0)12 5252 1500
Mobile: +44 (0) 79 6858 2121


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------



Gen3 Systems Limited Unit B2, Armstrong Mall Southwood Business Park Farnborough Hampshire GU14 0NR - UK ENGINEERING RELIABILITY IN ELECTRONICS Registered Number: 4639449 (England & Wales). Registered Office as above. DISCLAIMER : This message is intended only for the use of the individual or entity to which it is addressed and may contain information which is privileged, confidential, proprietary, or exempt from disclosure under applicable law. If you are not the intended recipient or the person responsible for delivering the message to the intended recipient, you are strictly prohibited from disclosing, distributing, copying, or in any way using this message. If you have received this communication in error, please notify the sender and destroy and delete any copies you may have received. Any views or opinions presented in this email are solely those of the author and might not represent those of Gen3 Systems Limited. Although Gen3 Systems Limited has taken reasonable precautions to ensure no viruses present in this email, Gen3 Systems Limited can not accept the responsibility for any loss or damage arising from the use of this email or attachments. On 31 Oct 2007, at 18:48, Guy Ramsey wrote: > In truth, it is my understanding that the flux was changed because > nobody > uses pure rosin flux anymore. They only reason the flux makers > produced it > was for solderability testing. > > The new flux specification was supposed to reflect real world > performance > requirements. We are using an L0 flux. But, I am sure it performs much > better, in the real world than the material specified in previous > revision > of the standard; False calls. > > Though, I suspect that someone using pure rosin flux could have > issues with > components that pass the current tests. > > Dave? > > -----Original Message----- > From: TechNet [mailto:[log in to unmask]] On Behalf Of Dennis Fritz > Sent: Wednesday, October 31, 2007 2:32 PM > To: [log in to unmask] > Subject: Re: [TN] Flux > > > Guys, > > I am vice chairman of the 5-23b committee on solderability with Dave > Hillman as the chairman. I do not officially remember why this was > changed, but it was for a reason - not willy-nilly. My suggestions > are > either: > 1. Because of some change in the J-004 standard on flux, or 2. The > changed > flux reduced the chance of false calls in the test. > > I have a reinforcing note to Dave Hillman to get you an answer. And, > please review the information still carried on the committee web site: > > _http://members.ipc.org/commReg/CommRegFile.asp? > PDFTYPE=min&ComName=Componen > t% > 20and%20Wire%20Solderability%20Specification%20T.G&comm=5-23B_ > (http://members.ipc.org/commReg/CommRegFile.asp? > PDFTYPE=min&ComName=Componen > t%20and%20Wire%20 > Solderability%20Specification%20T.G&comm=5-23B) > > From a quick scan, I don't see where this change is called out in the > minutes. Again, you can review most any of the IPC committtee > work, by > going as > follows: > > 1. IPC Web page > 2. Standards (that is under the Knowledge header) 3. Standards > Development > 4. Committee Home pages 5. Then, you have to be somewhat familiar > with the > IPC committee structure to know where to search. Assembly > standards tend to > all be under committee 5-20 Assembly and Joining. J-002 is under > Committee > 5-23B. > 6. Try it and you will like it (Dr. Suess). > > Denny Fritz > MacDermid, Inc. > > > In a message dated 10/31/2007 1:32:03 P.M. Eastern Daylight Time, > [log in to unmask] writes: > > New consensus . . . Who sits on these committees? > > -----Original Message----- > From: TechNet [mailto:[log in to unmask]] On Behalf Of Sue Powers- > Hartman > Sent: Wednesday, October 31, 2007 12:36 PM > To: [log in to unmask] > Subject: [TN] Flux > > The new JStd-002B 3.2.2 states that ROL1 flux shall be used for > solderability testing, while the old Rev JStd-002A 3.2.2 calls out > ROL0 > Flux. Does anyone know why this was changed? > > > > > > > ************************************** See what's new at http:// > www.aol.com > > --------------------------------------------------- > Technet Mail List provided as a service by IPC using LISTSERV 15.0 To > unsubscribe, send a message to [log in to unmask] with following text > in the > BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or > (re-start) delivery of Technet send e-mail to [log in to unmask]: SET > Technet > NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send > e-mail to [log in to unmask]: SET Technet Digest Search the archives of > previous posts at: http://listserv.ipc.org/archives Please visit > IPC web > site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional > information, or contact Keach Sasamori at [log in to unmask] or > 847-615-7100 > ext.2815 > ----------------------------------------------------- > > --------------------------------------------------- > Technet Mail List provided as a service by IPC using LISTSERV 15.0 > To unsubscribe, send a message to [log in to unmask] with following > text in > the BODY (NOT the subject field): SIGNOFF Technet > To temporarily halt or (re-start) delivery of Technet send e-mail > to [log in to unmask]: SET Technet NOMAIL or (MAIL) > To receive ONE mailing per day of all the posts: send e-mail to > [log in to unmask]: SET Technet Digest > Search the archives of previous posts at: http://listserv.ipc.org/ > archives > Please visit IPC web site http://www.ipc.org/contentpage.asp? > Pageid=4.3.16 for additional information, or contact Keach Sasamori > at [log in to unmask] or 847-615-7100 ext.2815 > ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------

ATOM RSS1 RSS2