TECHNET Archives

November 2006

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, "Dehoyos, Ramon" <[log in to unmask]>
Date:
Mon, 20 Nov 2006 14:27:25 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Wenger, George M." <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="us-ascii"
From:
"Wenger, George M." <[log in to unmask]>
Parts/Attachments:
text/plain (116 lines)
Crack at what interface?

Richard,


Ramon,



Crack at what interface?



Richard,



If "lead-rich zones within the finished solder joint that are

undesirable" what makes them undesirable in a SnPb solder joint?



-----Original Message-----

From: TechNet [mailto:[log in to unmask]] On Behalf Of Dehoyos, Ramon

Sent: Monday, November 20, 2006 1:50 PM

To: [log in to unmask]

Subject: Re: [TN] BGA anomaly



    The question is: are there 63/37 SnPb paste with flux that can

endure LF profiles? Or will the flux burn out and leave dull solder

joints?  SAC305 balls and 63/37 do not make reliable SJs. There is a

tendency to crack at the interface.

     Ramon 

 



-----Original Message-----

From: TechNet [mailto:[log in to unmask]] On Behalf Of Stadem, Richard D.

Sent: Monday, November 20, 2006 12:37 PM

To: [log in to unmask]

Subject: Re: [TN] BGA anomaly



Werner is correct, and my two cents worth; the profile must be of such

duration to ensure that the lead in the solder joint is properly

homogenized within the solder joint. Else you will have lead-rich zones

within the finished solder joint that are undesirable. 



-----Original Message-----

From: TechNet [mailto:[log in to unmask]] On Behalf Of Werner Engelmaier

Sent: Monday, November 20, 2006 9:06 AM

To: [log in to unmask]

Subject: Re: [TN] BGA anomaly



Hi Iain,

For a mixture of SnPb & PbF part (in particular PbF BGA's - SAC305)

using a

63/37 SnPb solder, the preferred reflow profile is definitely a LF-SAC

profile, NOT a SnPb-profile.



Werner



---------------------------------------------------

Technet Mail List provided as a service by IPC using LISTSERV 1.8e To

unsubscribe, send a message to [log in to unmask] with following text in

the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or

(re-start) delivery of Technet send e-mail to [log in to unmask]: SET

Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the

posts: send e-mail to [log in to unmask]: SET Technet Digest Search the

archives of previous posts at: http://listserv.ipc.org/archives Please

visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for

additional information, or contact Keach Sasamori at [log in to unmask] or

847-615-7100 ext.2815

-----------------------------------------------------



---------------------------------------------------

Technet Mail List provided as a service by IPC using LISTSERV 1.8e To

unsubscribe, send a message to [log in to unmask] with following text in

the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or

(re-start) delivery of Technet send e-mail to [log in to unmask]: SET

Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the

posts: send e-mail to [log in to unmask]: SET Technet Digest Search the

archives of previous posts at: http://listserv.ipc.org/archives Please

visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for

additional information, or contact Keach Sasamori at [log in to unmask] or

847-615-7100 ext.2815

-----------------------------------------------------



---------------------------------------------------

Technet Mail List provided as a service by IPC using LISTSERV 1.8e

To unsubscribe, send a message to [log in to unmask] with following text

in

the BODY (NOT the subject field): SIGNOFF Technet

To temporarily halt or (re-start) delivery of Technet send e-mail to

[log in to unmask]: SET Technet NOMAIL or (MAIL)

To receive ONE mailing per day of all the posts: send e-mail to

[log in to unmask]: SET Technet Digest

Search the archives of previous posts at:

http://listserv.ipc.org/archives

Please visit IPC web site

http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional

information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100

ext.2815

-----------------------------------------------------





------------------------------------------------------------------------------------------------

This message is for the designated recipient only and may

contain privileged, proprietary, or otherwise private information.  

If you have received it in error, please notify the sender

immediately and delete the original.  Any unauthorized use of

this email is prohibited.

------------------------------------------------------------------------------------------------

[mf2]



---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2