TECHNET Archives

November 2005

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Fri, 18 Nov 2005 13:31:19 -0600
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Content-type:
text/plain; charset=US-ASCII
Subject:
From:
"David D. Hillman" <[log in to unmask]>
X-cc:
In-Reply-To:
MIME-Version:
1.0
Parts/Attachments:
text/plain (86 lines)
Hi John! As an avid waterfowl hunter I can personally attest to the poor
ballistic properties of Bi shot - it works much better than steel shot but
the ammunition metallurgical folks are doing some pretty nifty things with
tungsten and other alloy combinations.

Dave Hillman
Rockwell Collins
[log in to unmask]



             John Maxwell
             <[log in to unmask]
             M>                                                         To
             Sent by: TechNet          [log in to unmask]
             <[log in to unmask]>                                          cc

                                                                   Subject
             11/18/2005 12:48          Re: [TN] EU Lead hysteria
             PM


             Please respond to
              TechNet E-Mail
                   Forum
             <[log in to unmask]>
             ; Please respond
                    to
               John Maxwell
             <[log in to unmask]
                    M>






ALLEN,
Actually most military bullets around the world use a steel core for
penetration. Either a gilding metal (cupre nickel) or iron/soft steel
jacket is used to protect the bore from the hardened steel core.
Bismuth has only been used in shot for water fowl but is being replace
by either iron or tungsten alloys for shot. Lead is still used as a
bullet core for most commercial rifle and pistol ammunition.

John Maxwell

>Bullets?
>
>The respectable Ms. Hwang indicates that bismuth has replaced lead in
>bullets -
>
>"Green bullets using Bi to replace Pb, making Pb-free combat-ready
>cartridges"
>
>fwiw
>
>Loa
>
>
>

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2