TECHNET Archives

November 2005

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Mon, 28 Nov 2005 10:49:44 -0600
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Content-type:
text/plain; charset=ISO-8859-1
Subject:
From:
"David D. Hillman" <[log in to unmask]>
X-cc:
In-Reply-To:
Content-transfer-encoding:
quoted-printable
MIME-Version:
1.0
Parts/Attachments:
text/plain (137 lines)
Hi Ramon! Nice logical flowdown for us "metrically impaired" engineers.

Dave Hillman
Rockwell Collins
[log in to unmask]



                                                                       
             "Dehoyos, Ramon"                                          
             <ramon.dehoyos@NG                                         
             C.COM>                                                     To
             Sent by: TechNet          [log in to unmask]                 
             <[log in to unmask]>                                          cc
                                                                       
                                                                   Subject
             11/28/2005 08:49          Re: [TN] Intermetallic Layer    
             AM                                                        
                                                                       
                                                                       
             Please respond to                                         
              TechNet E-Mail                                           
                   Forum                                               
             <[log in to unmask]>                                         
             ; Please respond                                          
                    to                                                 
             "Dehoyos, Ramon"                                          
             <ramon.dehoyos@NG                                         
                  C.COM>                                               
                                                                       
                                                                       




        1 micron = 1/1000000 of a Meter
        1 micron =   1/1000 of a mm
        1 mil =      1/1000 of in
        1 micro in = 1/1000 of a mill
        1 micro in = 1/1000000 of in
        1 mm = 1/25.4 in = 0.0393 in = 39.3 mils

                                   1 mm      1 in                 1000000
microns
        1 micron          X     ---------        X      ------     X
--------------  =  39.3 micro in
                              1000 microns      25.4 mm            in






-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Victor G. Hernandez
Sent: Monday, November 28, 2005 9:24 AM
To: [log in to unmask]
Subject: Re: [TN] Intermetallic Layer

I have been stating all along that MICRONS are a SMALLER unit of measure
than MICRO INCHES.

Victor,

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Indrek Rebane
Sent: Monday, November 28, 2005 7:56 AM
To: [log in to unmask]
Subject: Re: [TN] Intermetallic Layer

Hi Victor,

Victor G. Hernandez wrote:
> Microns are smaller units of measure than MICRO INCHES.

You seem to be confusing microinches with mils. One microinch is thousandth
of mil, which is thousandth of inch. One microinch is 0.0254 microns.

Indrek,
Actually a proponent of the SI (Metric) system.

--
Indrek Rebane
Borthwick-Pignon OÜ, R&D
Riia 185, 51014 Tartu, Estonia
Phone: +372 7 302 641, Fax: +372 7 383 041

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives Please visit IPC web
site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives Please visit IPC web
site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2