I have some questions about underfill.
1) I know that voids next to solder balls in underfills for flip chips
are no-nos because the pressure the cured underfill exerts on the solder
balls is enough to actually make them flow into the voids. My question
is: does this same concern exist for the larger solder balls of BGAs or
do they have enough strength to be resistant to this?
2) What do people allow for % voiding in underfills?
3) If a component has too many layers for acoustic microscopy to be used
and the underfill has no x-ray retarding character, how in the world
does one determine the amount of voiding in the underfill, short of
prying the part off the board?
4) What is the best course anyone has taken at APEX/SMTAI/ECTC, etc.
that was on underfilling or at least spent quite a bit of time on it?
5) Any particular book people would recommend?
Thanks.
Bev
RIM
---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|