TECHNET Archives

July 2005

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, "Black, Paul" <[log in to unmask]>
Date:
Fri, 22 Jul 2005 08:22:18 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Bev Christian <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="us-ascii"
From:
Bev Christian <[log in to unmask]>
Parts/Attachments:
text/plain (67 lines)
Paul,
Thicker board?  Nope.  Re-lay out a board?  For the latter I would have
to talk to a designer for sure, but I can tell you that by using
Thermoire we have found some boards and some parts with warpage - some
insignificant, some not. "It all depends".  Phrase either copyrighted or
trademarked by Doug Pauls. :)

Regards,
Bev

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Black, Paul
Sent: July 21, 2005 5:35 PM
To: [log in to unmask]
Subject: [TN] BGA's and Lead free

Hi Everyone,

We are starting to redesign a product for RoHS compliance and one of our
engineers has a concern. Due to the higher oven temps, he is afraid that
excess warpage may occur to the board and large components, particularly
the BGA's, and the resulting stress will lead to failures. He is
considering increasing the thickness of the board, which would be an
expensive proposition. Our largest BGA is a 19 x 19, 357 pin 1.27mm
pitch part on a 7" x 9" .062" board. I know that a number of you have
been working with lead free for a while. Have you had a need to increase
the thickness of the board?

Thank you, 
Paul Black 
Manufacturing Engineer 
Kronos 
E-mail: [log in to unmask] 

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------




---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2