Bev, because of the nutty nature of our business, we actually do this
frequently. I checked with my lead tech who is phenomenal at this sort of
thing and he suggests a simple solder bridge at the bend of the leads where
they intersect with the pad.
Bob Croslin
Nielsen Media Research
-----Original Message-----
From: Bev Christian [mailto:[log in to unmask]]
Sent: Thursday, January 16, 2003 2:01 PM
To: [log in to unmask]
Subject: [TN] Purposefully shorting two adjacent SOIC leads.
Technetters,
How do I do what is proposed in my title? The options are using excess
solder or using a mod wire. Are there other options for doing this mod?
What do people do? What is allowed and not allowed by IPC standards (I
couldn't find anything, but then I may not be looking in the right place.)
I would expect option one would be a whole heck of a lot easier than option
2. As long as option 1 doesn't produce bulbous joints with the solder all
the way up to the component body is there any real reason why I can't do
this?
regards,
Bev Christian
Research in Motion
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|