TECHNET Archives

February 2002

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Sat, 9 Feb 2002 14:29:43 EST
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset="US-ASCII"
From:
Parts/Attachments:
text/plain (28 lines)
Hi MoonCaveMan,
I had thought YOU had come out of your cave. I am currently babysitting for
my 3 granddaughters in NC.
Steve says: it is a 384-ball .8mm pitch PBGA with a heatslug on the top...
If it is in fact a PBGA with a heatslug on the top, than it is a SBGA--these
are notorious for warping when you change their temperature because they are
of a thermally asymetric design. I have seen solder balls ripped of the pads
and soldering pads ripped out of the PCB.
You could also be right about the silicone affecting the global expansion
mismatch with the PCB. TI has just agreed to license their microStarBGAs
under Tessera's patents to avoid infringement [Sharp's CSPs were found to
infringe Tessera's patents]. But it is not just CSPs that might have their
BLR affected by the die; larger BGAs that are thin can suffer from the same
problem.

Werner Engelmaier

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2