TECHNET Archives

February 2002

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Transfer-Encoding:
7bit
Sender:
Subject:
From:
Jorge Santana <[log in to unmask]>
Date:
Fri, 8 Feb 2002 10:58:59 -0600
Content-Type:
text/plain; charset="iso-8859-1"
MIME-Version:
1.0
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Jorge Santana <[log in to unmask]>
Parts/Attachments:
text/plain (48 lines)
Techneters

   How I can qualify a process involving different materials with different
CTEs.

   Scenario:
   One component soldered to the board with thermal bond underneath and
conformal coating

   This board will be outdoors and will face wide temperature range (
winters and summers )

   I don't have all numbers yet, but would like to known how to analyze them
when I got all info.

   CTE of the board ( metal substrate type board for better thermal transfer
characteristics )
   CTE of the solder joint
   CTE of the thermal compound underneath the part ( approximately 1 mil
thick )
   CTE of the conformal coating

  Tg of the board
  Tg of the solder joint
  Tg of the thermal compound
  Tg of the conformal coating

  Question :
   What is the safest CTE mismatch that would not affect solder joint
reliability ?

  Thanks for any advice.

Jorge Santana
Manufacturing / Process Engineer
LWT

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2