TGASIA Archives

November 2011

TGAsia@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Asia Committe Task Group Forum <[log in to unmask]>, Jim Wang <[log in to unmask]>
Date:
Tue, 1 Nov 2011 16:07:30 +0900
Reply-To:
Asia Committe Task Group Forum <[log in to unmask]>, shi hongbin <[log in to unmask]>
Message-ID:
Subject:
From:
shi hongbin <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="GB2312"
MIME-Version:
1.0
Parts/Attachments:
text/plain (64 lines)
JIS Z 3198-7 Test methods for lead-free solders --
Part 7: Method for shear strength of solder joints
on chip components

IEC/JEITA Standard
(Provisional title) Method for testing the side push
shear strength of soldered connections of surface mounted devices
using lead-free
solder

Similar Standards
SEMI G63-95 Test Method for Measurement of Die Shear Strength
JEITA ET-7403 Test methods of mechanical strength of surface mounting devices
JIS C0051 Environmental test methods - electrical, electronic - method
of testing terminal
strength

在 2011年11月1日 下午4:00,Jim Wang <[log in to unmask]> 写道:
> All
>
>
>
> 针对SMT小的Chip元件,在锡膏制程回流焊接后,是否在推力标准?
>
>
>
> Best Regards,
>
>
>
> Jim.Wang | QA Officer | Season Components Co., Ltd.
>
>
>
> Email address: [log in to unmask]
>
> Website address: http://www.seasongroup.com
>
> Tel:  (86) 769-8338-8030  Ext. 8018 or 13652594880
>
> Fax: (86) 769-8338-7427
>
> ______________________________________________________________________
> This email has been scanned by the MessageLabs Email Security System.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>



-- 
Best Regareds!
SHI Hongbin (史 洪賓)

------+------+------+------+------+------+------+------+------+------+------+------+------+------+------+------
TEL: 0081-080-3943-6281
Skype: hungpinshin
QQ: 59070371

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2