TECHNET Archives

July 2006

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Steve Gregory <[log in to unmask]>
Date:
Thu, 27 Jul 2006 08:55:01 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Schaefer, Chris" <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="iso-8859-1"
From:
"Schaefer, Chris" <[log in to unmask]>
Parts/Attachments:
text/plain (96 lines)
I agree with Steve. We use Kyzen A4520 @ 13% (125F) on boards processed with no-clean paste and 2% liquid flux. The results are great and since the change of chemistry and a new machine that has a level 4 chem. iso, I never here from the floor concerning white residues. Great huh? Now I can do more productive Engineering projects - one at a time. I have evaluated the A4630 and it works even better at lower temps., but I don't have the time to implement at this point. Kyzen is also working on a soap that would be used to remove water soluble fluxes at very low concentration, but I'm not sure if it is out yet. Note: this is not a sales generation of any sort - we just use their product.

Hope this helps.

CAS

Chris Schaefer
Suntron Corporation
Process Engineer
540 N. Rogers Road
Olathe, Kansas 66062
913.393.5878
[log in to unmask] 

NOTICE:
 
This message is intended for the use of the individual entity to which it is addressed and may contain information that is privileged, confidential and exempt from disclosure under applicable law. If the reader of this message is not the intended recipient, or the employee or agent responsible for delivering the message to the intended recipient, you are hereby notified that any dissemination, distribution or copying of this communication is strictly prohibited. If you have received this communication in error, please notify us immediately by calling 913.393.5878 or returning the original message to us.



-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Steve Gregory
Sent: Wednesday, July 26, 2006 3:25 PM
To: [log in to unmask]
Subject: Re: [TN] Water Cleaning No Clean FLux from a PCBA


Hi Michael!

From experience, Kyzen Aquanox XJN works very well on no-clean residues.
Kyzen also has newer formulas such as 4512P and 4520 that works even
better at lower concentrations. Any of the Aquanox family cleans
no-clean residues very well...

-Steve Gregory- 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Michael Forrester
Sent: Wednesday, July 26, 2006 3:15 PM
To: [log in to unmask]
Subject: [TN] Water Cleaning No Clean FLux from a PCBA

      We have a PCBA assembly that requires very low/none ionic
contamination due to high impedance circuitry.  Normally we use a water
soluble flux solder paste and wash the PCBAs.  Our current vendor only
uses Indium NC-SMQ92 no-clean solder paste.  To met the following spec:

Printed Circuit Assemblies shall meet cleanliness standards as per
IPC-A-610 and IPC/EIA J-STD-001.
Testing shall be in accordance with and meet the requirements of IPC/EIA
J-STD-001 Paragraph 8.3.6 or 8.3.7.

they want to use water and Kyzen XJN+ as a saponifier.  Has anyone used
this method of cleaning  a no clean assembly?  If so what was the
result?  Any other suggestions?
Thank you.

Best Regards,

Michael Forrester
Sr. Manufacturing Engineer
LeCroy Corp

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2