TECHNET Archives

May 2003

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Brian Ellis <[log in to unmask]>
Date:
Tue, 13 May 2003 23:33:14 -0700
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, BRAD VANDERHOOF <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset="iso-8859-1"
From:
BRAD VANDERHOOF <[log in to unmask]>
Parts/Attachments:
text/plain (105 lines)
Brian,

Back when I worked for a firm with some clout, this service was automatic.
As long as I placed orders they shipped the product to maintain the revenue
stream, no matter how many replacement products they had introduced.  Of
course we did buy direct and did not expect a stocking distributor to hold
obsolete product in inventory and patiently wait for an order.

Cheers,
Brad Vanderhoof
AITI


----- Original Message -----
From: "Brian Ellis" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Tuesday, May 13, 2003 3:56 AM
Subject: Re: [TN] Solder paste, why the secrecy?


> Steve
>
> One point I would consider when qualifying a product: a written
> guarantee by the vendor that the product will be on the market for a
> minimum of 5 years, preferably 10, without modification, so that you
> don't have to go to the expense of frequent requalification. In the
> event of a product being withdrawn within the period, for whatever
> reason, the vendor will support the cost of requalification, even if the
> results favour a competitor's product. If everyone insisted on this,
> then the manufacturer of the product will think twice about withdrawing
> a product during a viable lifetime. The downside, of course, is that,
> after 5 years, there may be better products on the market, but so what,
> if the one you are using does what you ask of it?
>
> Which large company with clout will start the ball rolling?
>
> Brian
>
> Steve Gregory wrote:
> > My latest post about Solder paste, has just raised an issue that I've
> > thought about over the years...this may upset some people.
> >
> > Why do us as users, need to go through all these qualification tests in
> > order to select a solder paste? All of us use the paste in the same way,
> > no? Aren't the vendors of these products AWARE of the requirements that
> > need to be met? Why don't they "tailor" their products to their users?
> > Do these vendors understand the expense and time that it takes to do all
> > these qualification tests? Why should we even have to do this? Don't
> > solder paste vendors understand their market?
> >
> > Even the IpC has put into place procedures to qualify solder paste. I
> > would think, that if I were a solder paste vendor, and to secure
> > business, I would make sure, that whatever product I sold, would comply
> > to all industry standards, and advertise it as such, and then back it
> > up...you would win market share with that simple effort.
> >
> > But to tell you the truth, I have recieved quite few emails that have
> > found that what was claimed, is not the truth...you have only yourself
> > to blame for that. So I will go on to do my own tests, and not even
> > consider your sales people and their pitches, because they lie to all of
> > us, and cannot be trusted...and that's a damn shame...
> >
> > -Steve Gregory-
> >
> > ---------------------------------------------------
> > Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
> > To unsubscribe, send a message to [log in to unmask] with following text
> > in the BODY (NOT the subject field): SIGNOFF Technet
> > To temporarily halt or (re-start) delivery of Technet send e-mail to
> > [log in to unmask]: SET Technet NOMAIL or (MAIL)
> > To receive ONE mailing per day of all the posts: send e-mail to
> > [log in to unmask]: SET Technet Digest
> > Search the archives of previous posts at:
http://listserv.ipc.org/archives
> > Please visit IPC web site http://www.ipc.org/html/forum.htm for
> > additional information, or contact Keach Sasamori at [log in to unmask] or
> > 847-509-9700 ext.5315
> > -----------------------------------------------------
>
> ---------------------------------------------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
> -----------------------------------------------------
>

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2