TECHNET Archives

January 1999

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
Subject:
From:
Guenter Grossmann <[log in to unmask]>
Date:
Fri, 22 Jan 1999 12:31:03 +0100
Content-Type:
text/plain; charset="us-ascii"
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Guenter Grossmann <[log in to unmask]>
Parts/Attachments:
text/plain (27 lines)
Hi all

I have a request of a company working with us. They face the problem that
their solder joints of QFP's on NiAu pad surfaces ( Au electroless plated )
does not bond in the reflow process. Trials have been made with various
suppliers of PCB's, all with the same result. All the other components seem
to solder Ok. Has somebody else gone through this? Does somebody know the
reason for the problem and maybe a solution?
Thanks for your help.

Best regards


Guenter

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2