Hi all I have a request of a company working with us. They face the problem that their solder joints of QFP's on NiAu pad surfaces ( Au electroless plated ) does not bond in the reflow process. Trials have been made with various suppliers of PCB's, all with the same result. All the other components seem to solder Ok. Has somebody else gone through this? Does somebody know the reason for the problem and maybe a solution? Thanks for your help. Best regards Guenter ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################