Nick and all,
We pre-tin our gold leads for the very same reasons you mention.
What do your customers say to the change?
Hans
Air Force Material Command - We keep them flying!
~~~~~~~~
Hans M. Hinners WR-ALC/LYPME Bldg. 640
Materials Engineer 380 Second Street,
Suite 104
Manufacturing Eng. Sec. Robins AFB GA 31098-1638
912-926-1970 (Voice) 468 - 1970 (DSN) 912-926-7974 (Fax)
[log in to unmask]
> -----Original Message-----
> From: Nick D'Onofrio [SMTP:[log in to unmask]]
> Sent: Tuesday, August 31, 1999 09:26
> To: [log in to unmask]
> Subject: [TN] Pre-tinning gold leads
> Importance: Low
>
> We are pre-tinning the gold leads prior to assembly on our military
> products. I'm looking for some constructive data or argument to decide if
> we
> should continue this practice.
> My concern would be gold embrittlement in the solder joint and any
> latent
> failures attributed to this.
> Any comments or guidance in this matter would appreciated.
>
> Regards,
> Nick D.
>
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|