In a former life, I used Alpha Metals WS-609, 90% metal and flux activity
ORH0. Dependent on your throughput, the only drawbacks are a 4 hour stencil
life and 6 hour tack time. A typical reflow profile is recommended with
time above liquidus to be 45 - 75 seconds. The flux residue can be easily
removed with 140°F water (w/o saponification) in a timely manner.
This paste formulation has been around for quite awhile. With that said,
there are probably other formulations that are available but I don't have
any personal experience with them as I have gone backwards in my career and
have been somewhat forced to use a RMA formulation.
Good luck with your search.
Steve Sauer
Sr. Manufacturing Engineer
Northrop Grumman, Electronic Systems
Xetron
Cincinnati, OH
-----Original Message-----
From: Marsico, James [mailto:[log in to unmask]]
Sent: Wednesday, October 20, 2004 2:07 PM
To: [log in to unmask]
Subject: [TN] solder paste
Hello Technet... My solder paste manufacturer, who shall remain nameless,
is discontinuing our presently used water soluble paste, so I'm looking for
a replacement. What seems to be the most widely used water soluble Sn63
solder paste these days?
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|