I agree with Phil and Peter, wholeheartedly. If the prepreg is a lo-flo
or no-flo type or if it has a low resin content (frequent with 7nnn
styles) or if the copper is thick or any combination of these, then you
are making a build-up which will be weakest exactly where you drill the
holes. The result will be ripe for many ills, and is a frequent
precursor to conductive anodic filaments (CAFs). With the copper in
place on every layer, you will have a nice, compact build-up.
Been there, done that!
Brian
Bill Decray wrote:
> Hello fellow TechNet Guru
> Does anyone have or know off any specifications that talk about removal of
> non functional pads and what effects it has on a finished circuit boards if
> any
>
>
>
> Highest Regards,
>
> William W. DeCray III
> Waytec Electronics Corp
> Engineering Services Manager
> PHONE:(434) 237-6391 ext 115
> CELL: (434) 851-6115
> FAX: (434) 237-1324
> E-mail:<[log in to unmask]>
> Web http://www.waytec.com
> FTP ftp://ftp.waytec.com
>
> ---------------------------------------------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
> -----------------------------------------------------
>
>
>
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|