TECHNET Archives

March 2003

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Michael Bell <[log in to unmask]>
Date:
Tue, 25 Mar 2003 10:27:20 +0200
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Brian Ellis <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset=us-ascii; format=flowed
From:
Brian Ellis <[log in to unmask]>
Parts/Attachments:
text/plain (72 lines)
Mike

The others have not really answered what roller tinning is. Imagine a
trough of molten solder, in which an iron drum is rotated with a
peripheral speed of about 10 or 15 cm/s. On top of the iron drum is a
heat-resistant "rubber" roller. The drum is tinned with the solder, with
the aid of an active water-soluble flux. The PCBs are dipped into the
same flux and fed between the drum and the roller, copper side down.
This transfers some of the tinning onto the copper. This is the basis of
roller tinning.

The thickness of the tinning is microscopic and is really only the
intermetallic layer with an admixture of iron, except that a blip of
thicker solder is left on the trailing edge of each conductor (much
worse than the uneveness of HASL). It was used for both single and
double (2 passages) sided circuits before plating-through of holes was
common, often the holes equipped afterwards with some form of rivet.
Obviously, it was useless with PTHs, because there was insufficient
tinning on the drum to enter the holes: this was the real cause for its
demise.

The quality of protection was fairly mediocre, solderability being
maintained for only 2 or 3 months, because of the thinness of the
coating. Notwithstanding, it was a very popular, cheap, coating in its
heyday. It was not replaced by HASL, which came later, but by tin-lead
plated boards initially, followed later by hot-oil and then infra-red
fusion. About the same timeas the late days of roller tinning was the
forerunner of HASL, the Hydrosqueegee. This called for passing the bare
boards over a solder wave and then immersing them in a violent spray of
hot oil to level off the excess and clear the holes, even PTH. This was
not very popular because the smell was atrocious and the machines were a
fire hazard.

Brian

Michael Bell wrote:
> Hi all,
>
> Just a little stumped on terminology here, what is "Roller Tinning".  What
> is the specific differences between this method and HASL???  Are there any
> specific pros/cons for the Roller method???  Any information would be
> appreciated.
>
> Cheers
>
> Mike
>
> ---------------------------------------------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
> -----------------------------------------------------
>
>
>

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2