TECHNET Archives

November 2006

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Wenger, George M." <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Wenger, George M.
Date:
Mon, 27 Nov 2006 13:06:44 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (306 lines)
Look at my 3b.  We don't subject SnPb components to Pb-Fr
Ramon,



Look at my 3b.  We don't subject SnPb components to Pb-Free reflow

profiles.  When we have to do a mixed alloy assembly we elect to run at

the upper end (225-230C) of a SnPb profile. 





Regards, 

George 

George M. Wenger 

Senior Principle FMA / Reliability Engineer 

Wireless network Solutions 

Andrew Corporation, 40 Technology Drive, Warren, NJ 07059 (908) 546-4531

[log in to unmask] 





-----Original Message-----

From: Dehoyos, Ramon [mailto:[log in to unmask]] 

Sent: Monday, November 27, 2006 12:09 PM

To: TechNet E-Mail Forum; Wenger, George M.

Subject: RE: [TN] FW: [TN] BGA anomaly





	George:

		 Isn't the trade off of  avoiding the reballing for the

2 & 3 reasons not outweigh the risk of taking the other components to LF

profiles? I would say that if all the components are capable

withstanding that temp, it would definitely work. All the components

must be made to be processed in LF profiles. How about if the process is

using SnPb solder and to use SnPb profiles. Would you recommend to

reball? My apologies for all these questions. I am sure others would

like to hear also.

	Regards,	

	Ramon



-----Original Message-----

From: TechNet [mailto:[log in to unmask]] On Behalf Of Wenger, George M.

Sent: Monday, November 27, 2006 9:00 AM

To: [log in to unmask]

Subject: Re: [TN] FW: [TN] BGA anomaly



There are three issues with re-balling BGA's:

1. It

Ramon,



There are three issues with re-balling BGA's:

1. It is expensive

2. You void the component manufacturers warranty 3. It is a solder

repair/replacement process that requires two heating operations(removal

and Replacement)



The reason we do not re-ball is because of 2 & 3.  Anytime you do a

repair process you can introduce reliability issues and when it is

compounded by losing the warranty we decided not to reball 





Regards,

George

George M. Wenger

Senior Principle FMA / Reliability Engineer Wireless network Solutions

Andrew Corporation, 40 Technology Drive, Warren, NJ 07059 (908) 546-4531

[log in to unmask] 





-----Original Message-----

From: TechNet [mailto:[log in to unmask]] On Behalf Of Dehoyos, Ramon

Sent: Monday, November 27, 2006 8:47 AM

To: [log in to unmask]

Subject: Re: [TN] FW: [TN] BGA anomaly



        Hi George:

                    " c). Do not re-ball Pb-Free area array packages

with SnPb balls."



  

        Do you recommend not to reball SAC balls even if the solder

paste to be used is SnPb and Pb profiles? Could you expand the matter?

Thanks for your inputs.

        Regards,

        Ramon

 



-----Original Message-----

From: TechNet [mailto:[log in to unmask]] On Behalf Of Braddock, Iain

Sent: Monday, November 27, 2006 4:57 AM

To: [log in to unmask]

Subject: Re: [TN] FW: [TN] BGA anomaly



Many thanks all for your responses, the team have come good again! 



I guess I wasn't far off the mark then, looks like some discussions with

the Design Team are order of the day!



Regards,

        Iain.



-----Original Message-----

From: Wenger, George M. [mailto:[log in to unmask]]

Sent: 24 November 2006 15:49

To: TechNet E-Mail Forum; Braddock, Iain

Subject: RE: [TN] FW: [TN] BGA anomaly





Iain,



You've stated correctly the dilemma companies are facing.  You've

comment/question about option 2 creating a reliability concern and also

invalidating the manufacturers warranty is also correct.  Companies are

going to have to make their own risk assessments.  Unfortunately, many

of those decisions are not knowledge based decisions because there isn't

good documented information available. The recommendations I've made

internally are:



1. Use SnPb assembly whenever possible

2. Use Pb-Free components and processes when product needs to be RoHS

6/6 compliant.

3. When forced into mixed alloy assembly:

        a. For RoHS 6/6 product, use Pb-Free processes (245-260C) when

all             components are compatible with Pb-Free processes.

        b). For RoHS 5/6 product, use maximum SnPb process temperatures

(225-           235C) whenever there are components not compatible with

Pb-Free                 processes (i.e., don't exceed the maximum

temperature the MSL             was tested at by the component vendor.

        c). Do not re-ball Pb-Free area array packages with SnPb balls.



Regards,

George

George M. Wenger

Andrew Corporation Wireless Network Solutions Senior Principal FMA /

Reliability Engineer 40 Technology Drive, Warren, NJ 07059

(908) 546-4531 [Office]  (732) 309-8964 [Cell] -----Original

Message-----

From: TechNet [mailto:[log in to unmask]] On Behalf Of Braddock, Iain

Sent: Friday, November 24, 2006 7:43 AM

To: [log in to unmask]

Subject: Re: [TN] FW: [TN] BGA anomaly



This sure is an interesting dilemma!



So which is the lesser of the two evils assuming you are forced into it

with the Design?



        1)      SnPb / SAC BGA's with a temperature profile (230ish)

that allows all joints to go liquidus.

        2)      Reball SAC BGA's with SnPb balls & use standard SnPb

thermal profile.



If option 2 does that not create reliability concerns also invalidate

the manufacturers warranty?



Regards,

        Iain.



-----Original Message-----

From: TechNet [mailto:[log in to unmask]]On Behalf Of Werner Engelmaier

Sent: 22 November 2006 17:39

To: [log in to unmask]

Subject: Re: [TN] FW: [TN] BGA anomaly





               *** WARNING ***



This mail has originated outside your organization, either from an

external partner or the Global Internet. 

     Keep this in mind if you answer this message. 



Hi Ramon,

Mixing SnPb with SAC is not a very good idea--you are right.







Werner



---------------------------------------------------

Technet Mail List provided as a service by IPC using LISTSERV 1.8e To

unsubscribe, send a message to [log in to unmask] with following text in

the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or

(re-start) delivery of Technet send e-mail to

[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing

per day of all the posts: send e-mail to

[log in to unmask]: SET Technet Digest

Search the archives of previous posts at:

http://listserv.ipc.org/archives

Please visit IPC web site

http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional

information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100

ext.2815

-----------------------------------------------------





********************************************************************

This email and any attachments are confidential to the intended

recipient and may also be privileged. If you are not the intended

recipient please delete it from your system and notify the sender.

You should not copy it or use it for any purpose nor disclose or

distribute its contents to any other person.

********************************************************************



---------------------------------------------------

Technet Mail List provided as a service by IPC using LISTSERV 1.8e To

unsubscribe, send a message to [log in to unmask] with following text in

the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or

(re-start) delivery of Technet send e-mail to

[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing

per day of all the posts: send e-mail to

[log in to unmask]: SET Technet Digest

Search the archives of previous posts at:

http://listserv.ipc.org/archives

Please visit IPC web site

http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional

information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100

ext.2815

-----------------------------------------------------





------------------------------------------------------------------------

------------------------

This message is for the designated recipient only and may contain

privileged, proprietary, or otherwise private information.  

If you have received it in error, please notify the sender immediately

and delete the original.  Any unauthorized use of this email is

prohibited.

------------------------------------------------------------------------

------------------------

[mf2]





********************************************************************

This email and any attachments are confidential to the intended

recipient and may also be privileged. If you are not the intended

recipient please delete it from your system and notify the sender.

You should not copy it or use it for any purpose nor disclose or

distribute its contents to any other person.

********************************************************************



---------------------------------------------------

Technet Mail List provided as a service by IPC using LISTSERV 1.8e To

unsubscribe, send a message to [log in to unmask] with following text in

the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or

(re-start) delivery of Technet send e-mail to [log in to unmask]: SET

Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the

posts: send e-mail to [log in to unmask]: SET Technet Digest Search the

archives of previous posts at: http://listserv.ipc.org/archives Please

visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for

additional information, or contact Keach Sasamori at [log in to unmask] or

847-615-7100 ext.2815

-----------------------------------------------------



---------------------------------------------------

Technet Mail List provided as a service by IPC using LISTSERV 1.8e To

unsubscribe, send a message to [log in to unmask] with following text in

the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or

(re-start) delivery of Technet send e-mail to [log in to unmask]: SET

Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the

posts: send e-mail to [log in to unmask]: SET Technet Digest Search the

archives of previous posts at: http://listserv.ipc.org/archives Please

visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for

additional information, or contact Keach Sasamori at [log in to unmask] or

847-615-7100 ext.2815

-----------------------------------------------------

------------------------------------------------------------------------

------------------------

This message is for the designated recipient only and may contain

privileged, proprietary, or otherwise private information.  

If you have received it in error, please notify the sender immediately

and delete the original.  Any unauthorized use of this email is

prohibited.

------------------------------------------------------------------------

------------------------

[mf2]





---------------------------------------------------

Technet Mail List provided as a service by IPC using LISTSERV 1.8e To

unsubscribe, send a message to [log in to unmask] with following text in

the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or

(re-start) delivery of Technet send e-mail to [log in to unmask]: SET

Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the

posts: send e-mail to [log in to unmask]: SET Technet Digest Search the

archives of previous posts at: http://listserv.ipc.org/archives Please

visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for

additional information, or contact Keach Sasamori at [log in to unmask] or

847-615-7100 ext.2815

-----------------------------------------------------



------------------------------------------------------------------------------------------------

This message is for the designated recipient only and may

contain privileged, proprietary, or otherwise private information.  

If you have received it in error, please notify the sender

immediately and delete the original.  Any unauthorized use of

this email is prohibited.

------------------------------------------------------------------------------------------------

[mf2]



---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2