Try print, then dispense glue, p/p and
reflow. Glue will freeze components prior reflow. If this is too
much hassle for you, tinker with your temp profile. A slower
heat absorption rate provides a better heat distribution and
equilibrium, so tombstoning phenomenon will be reduced.
M. Park
>>> <[log in to unmask]> January 14, 1998
8:12 am >>>
We have been experiencing problems with tombstoning of
1210 caps. I
have not been able to find any information about parts this
large
tombstoning. Is there any way to fix this problem while
we are
waiting for a design change to the pad layout?
Any help on this subject will be greatly appreciated.
Sean Gearin
[log in to unmask]
##############################################################
TechNet Mail List provided as a free service by IPC using
LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to
[log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm)
for additional information.
For the technical support contact Dmitriy Sklyar at
[log in to unmask] or 847-509-9700 ext.311
##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################
|
|
|