TECHNET Archives

April 2003

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
"TechNet E-Mail Forum." <[log in to unmask]>, "Peter L." <[log in to unmask]>
Date:
Mon, 7 Apr 2003 15:48:50 -0400
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, "Morse, Carrie" <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="iso-8859-1"
From:
"Morse, Carrie" <[log in to unmask]>
Parts/Attachments:
text/plain (49 lines)
Are these DPAK style components?
If so, you can print paste but, may find it does "droop" out.
What we have found works is to mask of those locations on the
bottom with Kapton tape.  Print and reflow.  Remove the tape prior
to wash if using OA.

-----Original Message-----
From: Peter L. [mailto:[log in to unmask]]
Sent: Monday, April 07, 2003 2:19 PM
To: [log in to unmask]
Subject: [TN] Filling PTH with solder


Technet,

What's the best method to solder fill 0.052" PTHs on a single sided SMT pcb
assembly? There are several of them on the board and some will be covered
by the body of large SMT inductors with no standoff.

There is no solder mask on the bottom side and I would not want to create
additional wave process. And on the open PTHs with this size, will stencil
printing create any paste "drooping" through the bottom side?


Rgds,
Peter

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2