TECHNET Archives

July 1998

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Type:
text/plain
Sender:
Subject:
From:
"Cash, Alan" <[log in to unmask]>
Date:
Fri, 31 Jul 1998 09:57:16 -0400
MIME-Version:
1.0
X-To:
Dave Thomas <[log in to unmask]>
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, "Cash, Alan" <[log in to unmask]>
Parts/Attachments:
text/plain (89 lines)
     Silicone grease migrating onto an existing solder joint may render
the joint difficult or impossible to resolder during a rework operation.
The grease may also migrate from the PWA to containers, bags, and/or
work surfaces which in turn may affect material coming in contact with
those items.

     Al Cash

> ----------
> From:         Dave Thomas[SMTP:[log in to unmask]]
> Reply To:     TechNet E-Mail Forum.;Dave Thomas
> Sent:         Friday, July 31, 1998 6:01 AM
> To:   [log in to unmask]
> Subject:      [TN] Silicone grease around soldered joints!
>
> People
>
> I am looking for some assistance in justifying the non-use of silicone
> grease, ie Dow Corning 304, near soldered joints.
>
> Could someone please supply me with a route to suitable
> documentation/reports to support this?
>
> I understand that if silicone grease should get on a joint prior to
> soldering, there is a very good chance thatthe soldering process will
> be
> faulty. I am not so clear as to long term effects of silicone grease
> maybe
> migrating into soldered joints causing degredation and failure in
> service.
>
> The manufacturing site I am currently working with are unhappy about
> having
> silicone grease in their factory so I am having to find suitable
> alternatives. The difficulty is that my engineers are more than happy
> with
> silicone, but do not have to worry about long term effects.
>
> Your help would be appreciated.
>
>
> Regards
>
> Dave Thomas
>
> Nothing will ever be attempted, if all possible objections must
> first be overcome.
>
> -- Samuel Johnson, "Rasselas", 1759
>
> ===============================================================
> Dave Thomas                                     Nortel plc
> Principal NPI Engineer,                         London Road
> European Radio                          Harlow
>                                         Essex
> Telephone:      +44 1279 402901                 CM17 9NA
> Facsimile:      +44 1279 402100                 UK
> ESN:    742-2901
> E-mail: [log in to unmask]
> ===============================================================
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV
> 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in the body:
> To subscribe:   SUBSCRIBE TechNet <your full name>
> To unsubscribe:   SIGNOFF TechNet
> ################################################################
> Please visit IPC's web site (http://www.ipc.org) "On-Line Services"
> section for additional information.
> For technical support contact Hugo Scaramuzza at [log in to unmask] or
> 847-509-9700 ext.312
> ################################################################
>

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2