Dave,
If the purpose of the grease is thermal transfer, there are alternatives
(sil-pads, etc.) that are much less messy, even if silicone is not the
issue.
Ralph Vaughan
Boeing
> ----------
> From: Dave Thomas[SMTP:[log in to unmask]]
> Reply To: TechNet E-Mail Forum.;Dave Thomas
> Sent: Friday, July 31, 1998 6:01 AM
> To: [log in to unmask]
> Subject: [TN] Silicone grease around soldered joints!
>
> People
>
> I am looking for some assistance in justifying the non-use of silicone
> grease, ie Dow Corning 304, near soldered joints.
>
> Could someone please supply me with a route to suitable
> documentation/reports to support this?
>
> I understand that if silicone grease should get on a joint prior to
> soldering, there is a very good chance thatthe soldering process will be
> faulty. I am not so clear as to long term effects of silicone grease maybe
> migrating into soldered joints causing degredation and failure in service.
>
> The manufacturing site I am currently working with are unhappy about
> having
> silicone grease in their factory so I am having to find suitable
> alternatives. The difficulty is that my engineers are more than happy with
> silicone, but do not have to worry about long term effects.
>
> Your help would be appreciated.
>
>
> Regards
>
> Dave Thomas
>
> Nothing will ever be attempted, if all possible objections must
> first be overcome.
>
> -- Samuel Johnson, "Rasselas", 1759
>
> ===============================================================
> Dave Thomas Nortel plc
> Principal NPI Engineer, London Road
> European Radio Harlow
> Essex
> Telephone: +44 1279 402901 CM17 9NA
> Facsimile: +44 1279 402100 UK
> ESN: 742-2901
> E-mail: [log in to unmask]
> ===============================================================
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in the body:
> To subscribe: SUBSCRIBE TechNet <your full name>
> To unsubscribe: SIGNOFF TechNet
> ################################################################
> Please visit IPC's web site (http://www.ipc.org) "On-Line Services"
> section for additional information.
> For technical support contact Hugo Scaramuzza at [log in to unmask] or
> 847-509-9700 ext.312
> ################################################################
>
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|