Well sumxp,
Your PCB supplier is telling you the truth and your customer is probably
telling what he knows (who knows if he knows the truth).
But this may be " A FAILURE TO COMMUNICATE". If the customer is saying
that he needs 50 ohms +/- 5% for the RF board that is different than trace
width +/- 5%. But +/- 20% control on trace width will NOT get you
impedance at +/- 5%, +/- 10% YES, but not 5%.
Below is our measurements in fabrication of the various contributions to
final impedance. You can see how important thickness control is. In
order to build RamBus, many had to learn how to control impedance to +/-
2.8 ohms, but in doing so ALL fabrication and material tolerances had to
be improved. The list of what it takes for fabrication tolerances for
final impedances from +/- 10% to +/-5% is below:
Happy Holden
Asian Pacific Materials
sumxp <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
09/04/2005 02:30 AM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
sumxp <[log in to unmask]>
To
[log in to unmask]
cc
Subject
[TN] 5% trace width control_RF
My customer told me that one of the RF pcb need to maintain the 5mils
trace
width within 5% tolerance in order to achieve 50 ohms impedance.
My pcb maker said they can only control at 20%(copper etching process
capability) trace width tolerance BUT can guarantee that the impedance is
at 50 ohms.
Please comment.Should I take the words of pcb supplier?
rgds
sumxp
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
|
|
|