So Thermoset was no good then? Suggest go up a rung in the feeding chain:
Have you tried the bigger chemical polymer houses like GE, Dow, Henkel and so on?
[Might be difficult if you want less than 200L/54USG/45IMPG drums mind!] and work down again
Mike
----- Original Message -----
From: Paul Klasek <[log in to unmask]>
To: <[log in to unmask]>
Sent: Tuesday, April 18, 2000 7:04 AM
Subject: [TN] Foamed Silicon
> Dear Netties ,
> i'm seriously stuck here ;
> could any of you spare me ANY lead (non Pb) to foamed flexible silicon
> please :
>
> the target is hydrolysis
> (humidity/temperature aging, of foamed polyurethanes for example)
> resistant flexible foam , inject mouldable to curing dies ;
> about 50 grams shot size (a handful, 6"ball)
>
> Technology, equipment, sheet/block fabricators, .......
>
> The foamed silicon lasts for a century ; unlike pu for less than decade .
>
> I
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
|
|
|