TECHNET Archives

April 2000

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Paul Klasek <[log in to unmask]>
Date:
Tue, 18 Apr 2000 17:40:38 +0100
Reply-To:
Michael Fenner <[log in to unmask]>
Subject:
From:
Michael Fenner <[log in to unmask]>
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset="iso-8859-1"
Organization:
Bonding Services & Products
MIME-Version:
1.0
Parts/Attachments:
text/plain (43 lines)
So Thermoset was no good then? Suggest go up a rung in the feeding chain:
Have you tried the bigger chemical polymer houses like GE, Dow, Henkel and so on?
[Might be difficult if you want less than 200L/54USG/45IMPG drums mind!] and work down again

Mike

----- Original Message -----
From: Paul Klasek <[log in to unmask]>
To: <[log in to unmask]>
Sent: Tuesday, April 18, 2000 7:04 AM
Subject: [TN] Foamed Silicon


> Dear Netties ,
> i'm seriously stuck here ;
> could any of you spare me ANY lead (non Pb) to foamed flexible silicon
> please :
>
> the target is hydrolysis
> (humidity/temperature aging, of foamed polyurethanes for example)
> resistant flexible foam , inject mouldable to curing dies ;
> about 50 grams shot size (a handful, 6"ball)
>
> Technology, equipment, sheet/block fabricators, .......
>
> The foamed silicon lasts for a century ; unlike pu for less than decade .
>
> I

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################

ATOM RSS1 RSS2