At 02:21 PM 8/7/2012, Phil Bavaro wrote:
>I used to do a lot of pin in paste on connectors but it has been long
>enough that I cannot remember if I eliminated the voiding completely or
>not. My memory says that I achieved the 75% and did not have
>unacceptable voiding.
the older you get, the better you were.
> I remember the worst part of PIP was the dragout
>problem of inserting the pins through the solder paste and dripping on
>the placement equipment. Don't have an documents to refer you to
>offhand. Dean's honeycomb pre-forms sounds like a proven method albeit
>more costly.
>
>-----Original Message-----
>From: TechNet [mailto:[log in to unmask]] On Behalf Of Stadem, Richard D.
>Sent: Tuesday, August 07, 2012 2:16 PM
>To: [log in to unmask]
>Subject: Re: [TN] pin in paste
>
>Hi, Joyce.
>Sorry, I tried different methods using paste and different brands of
>paste (including pre-drying) on connector pins but could not escape the
>voids entirely. Pre-drying the paste after insertion/before reflow did
>reduce the voiding, but was not practical from an assembly standpoint. I
>ended up using honeycomb (daisychain) pre-forms, with absolutely no
>voiding but a few minutes of added assembly time. If anyone else has
>ideas, I also would like to hear about them.
>
>-----Original Message-----
>From: TechNet [mailto:[log in to unmask]] On Behalf Of Joyce Koo
>Sent: Tuesday, August 07, 2012 4:04 PM
>To: [log in to unmask]
>Subject: [TN] pin in paste
>
>Joyce Koo
>Materials Researcher - Materials Interconnect Lab Research In Motion
>Limited
>Office: (519) 888-7465 79945
>Mobile: (226) 220-4760
>
>Hi, Calling on all of the gurus, Anyone has one or two good reference
>regarding voiding minimization or voiding elimination for pin in paste?
>Hopefully it is not in need of using performs. Many thanks for all your
>help.
>Best regards,
> joyce
>
>---------------------------------------------------------------------
>This transmission (including any attachments) may contain confidential
>information, privileged material (including material protected by the
>solicitor-client or other applicable privileges), or constitute
>non-public information. Any use of this information by anyone other than
>the intended recipient is prohibited. If you have received this
>transmission in error, please immediately reply to the sender and delete
>this information from your system. Use, dissemination, distribution, or
>reproduction of this transmission by unintended recipients is not
>authorized and may be unlawful.
>
>______________________________________________________________________
>This email has been scanned by the Symantec Email Security.cloud
>service.
>For more information please contact helpdesk at x2960 or
>[log in to unmask]
>______________________________________________________________________
>
>______________________________________________________________________
>This email has been scanned by the Symantec Email Security.cloud
>service.
>For more information please contact helpdesk at x2960 or
>[log in to unmask]
>______________________________________________________________________
>
>------------------------------------------------------------------------------
>This message and any attachments are solely for the use of the
>addressee and may contain L-3 proprietary information that may also
>be defined as USG export controlled technical data. If you are not
>the intended recipient, any disclosure, use or distribution of its
>content is prohibited. Please notify the sender by reply e-mail and
>immediately delete this message and any attachments.
>
>
>
>
>______________________________________________________________________
>This email has been scanned by the Symantec Email Security.cloud service.
>For more information please contact helpdesk at x2960 or [log in to unmask]
>______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|